Soft vs. Hard Piezo Ceramics

Small amounts of a donor dopant added to a ceramic formulation create metal (cation) vacancies in the crystal structure, enhancing the effects of extrinsic factors on the piezoelectric properties of the ceramic. The products of such formulations – soft ceramics – are characterized by large electromechanical coupling factors, large piezoelectric constants, high permittivity, large dielectric constants, high dielectric losses, low mechanical quality factors, and poor linearity. Soft ceramics produce larger displacements and wider signal band widths, relative to hard ceramics, but they exhibit greater hysteresis, and are more susceptible to depolarization or other deterioration. Lower Curie points (generally below 300°C) dictate that soft ceramics be used at lower temperatures. Generally large values for permittivity and dielectric dissipation factor restrict or eliminate soft ceramics from applications requiring combinations of high frequency inputs and high electric fields. Consequently, soft ceramics are used primarily in sensing applications, rather than in power applications.

An acceptor dopant in a ceramic formulation creates oxygen (anion) vacancies in the crystal structure. Hard ceramics have characteristics generally opposite those of soft ceramics, including Curie points above 300°C, small piezoelectric charge constants, large electromechanical coupling factors, and large mechanical quality factors. They also are more difficult to polarize or depolarize. Although hard ceramics generally are more stable than soft ceramics, they cannot produce the same large displacements. Hard ceramics are compatible with high mechanical loads and high voltages.

Be aware, however, that a soft ceramic can be prepared to exhibit some characteristics approaching those of a hard ceramic, or vice versa. Thus, when choosing a ceramic for a particular application, it can be useful to look beyond general categorization, and carefully compare specific characteristics.

Request a Quote

Characteristics of Soft Ceramics and Hard Ceramics Compared

Explore Our Additional Resources:

Testing and Packing PZT Ceramics

Poling PZT Ceramics

Electroding PZT Ceramics

Machining PZT Ceramics

Soft vs. Hard Piezo CeramicsFor much more information about piezoelectric ceramics and their uses, order our book: 

Piezoelectric Ceramics: Principles and Applications

 

a white background with a few lines on it

Contact APC International Today to Discuss Your Piezoelectric Ceramic or Piezo Device Requirements

Have questions about APC International’s piezo products? Contact us or call us at (570)726-6961 to learn more information.

Request a Quote