Influence of Input Frequency
At low input frequencies, the relationships between a force applied to a piezoelectric ceramic element and the electric field or charge produced by the piezo element are:
E = -(g33T)
Q = -(d33F)
whereE: electric field
g33: piezoelectric voltage constant
T: stress on ceramic element
Q: generated charge
d33: piezoelectric charge constant
F: applied force
The relationships between an applied voltage or electric field and the corresponding increase or decrease in a piezoelectric ceramic element’s thickness, length, or width are:
Δh = d33V
S = d33E
Δl / l = d31E
Δw / w = d31E
where l: initial length of ceramic element
w: initial width of ceramic element
Δh: change in height (thickness) of ceramic element
Δl: change in length of ceramic element
Δw: change in width of ceramic element
d: piezoelectric charge constant
V: applied voltage
S: strain (change in height / original height of element)
E: electric field