Piezoelectric Tolerences

Standard Machining Tolerances for APCI Ceramic Parts

 
Nominal Value
Standard Tolerance (±)
Disc/Ring/Cylinder (Tube): Outer Diameter
<1.000″ 0.010″
≥1.000″ to <1.500″ 0.015″
≥1.500″ to <2.000″ 0.025″
≥2.000″ 0.040″
<25 mm 0.25 mm
≥25 mm to <38 mm 0.38 mm
≥38 mm to <50 mm 0.60 mm
≥50 mm 1.00 mm
Ring/Cylinder (Tube): Inner Diameter
<0.250″ 0.010″
≥0.250″ to <0.500″ 0.015″
≥0.500″ to <1.000″ 0.020″
≥1.000″ 0.025″
<6 mm 0.25 mm
≥6 mm to <13 mm 0.38 mm
≥13 mm to <25 mm 0.50 mm
≥25 mm 0.60 mm
Plate: Length or Width
<0.500″ 0.005″
≥0.500″ to <1.000″ 0.010″
≥1.000″ to <1.500″ 0.015″
≥1.500″ to <2.000″ 0.025″
≥2.000″ 0.040″
<13 mm 0.13 mm
≥13 mm to <25 mm 0.25 mm
≥25 mm to 38 mm 0.38 mm
≥38 mm to <50 mm 0.60 mm
≥50 mm 1.00 mm
All Parts: Thickness
0.008″ to <0.200″ 0.001″
≥0.200″ 0.002″
0.20 mm to <5.00 mm 0.025 mm
≥5.00 mm 0.05 mm

Permissible Irregularities

Irregularity Linear Std. Dimen. Allowable Size Linear Metric Dimen. Allowable Size
Physical Chips <0.250″ ≤0.040″ <6.35mm ≤1.00mm
  ≥0.250″ <0.500″ ≤0.080″ ≥6.35mm <13.00mm ≤2.00mm
  ≥0.500″ <1.000″ ≤0.100″ ≥13.00mm <25.00mm ≤2.50mm
  ≥1.000″ ≤0.125″ ≥25.00mm ≤3.17mm
Silver Flaws
Total combined area of silver flaws is not to exceed 0.5% of total electrode area
Cracks
Parts are to be free of cracks
Standard physical inspections are performed with no magnification, roughly 12″ from workspace

We will attach electrical leads on request. Common leads are:

  • 26AWG to 32AWG / ranging from 2″ to 6″ in length
  • Stock size is 32AWG / 6″ in length
  • Other sizes are available upon request

Please be specific when requesting parts, tolerances, or electrode patterns. Provide drawings or sketches for parts or electrode patterns, and include ID tolerance if requesting rings or cylinders (tubes). For custom electrical leads, please specify AWG and length and provide a drawing showing the desired locations.