Single PZT layer (Unimorph) / solid electrode or two PZT layers / solid electrode. Additional data available on request.
Other units are available on request – please inquire.
* Input voltage (Vp-p max): 30
Typical Temperature Specification:
Typical Use Temperature: -20C to +50C
Typical Storage Temperature: -20C to +70C
Input voltage (Vp-p max): 15
We can design and produce disc benders for unique requirements. If the design you need is not listed here, please contact an APCI representative to discuss your specifications. Please see our Construction Options for custom disc benders.
APC also produces piezo discs, rings, and plates. APC will bond piezo elements to matching layers upon request.