Ready to Deliver Piezoelectric Ceramics
Fast Delivery Available! One Week or Sooner!
Clearance PZT Piezo Shapes
Item | Shape | Outer Diameter or Length | Inner Diameter or Width | THK/Cylinder LN | Material | Electrode Pattern | Price/Each | Quantity Available |
---|---|---|---|---|---|---|---|---|
956 | Cylinder | 19.00 mm | 15.80 mm | 5.60 mm | 840 | Solid | $25.00 | 58 |
2475 | Cylinder | 19.00 mm | 15.90 mm | 5.60 mm | 840 | Solid | $25.00 | 19 |
2472 | Cylinder | 19.00 mm | 15.90 mm | 5.50 mm | 840 | Solid | $25.00 | 8 |
2476 | Cylinder | 19.10 mm | 15.90 mm | 5.60 mm | 840 | Solid | $25.00 | 18 |
2317 | Cylinder | 15.20 mm | 9.80 mm | 5.00 mm | 841 | Solid | $25.00 | 22 |
1448 | Disc | 3.20 mm | 1.50 mm | 840 | Solid | $12.00 | 83 | |
1351 | Disc | 5.10 mm | 0.40 mm | 840 | Solid | $12.00 | 968 | |
1440 | Disc | 6.40 mm | 1.10 mm | 840 | Solid | $12.00 | 206 | |
1445 | Disc | 7.10 mm | 6.80 mm | 840 | Tab | $12.00 | 6 | |
1352 | Disc | 7.50 mm | 0.80 mm | 840 | Solid | $12.00 | 44 | |
62 | Disc | 7.60 mm | 0.25 mm | 840 | Solid | $12.00 | 31 | |
1079 | Disc | 7.60 mm | 0.25 mm | 840 | Solid | $12.00 | 120 | |
1444 | Disc | 8.00 mm | 8.00 mm | 840 | Solid | $12.00 | 7 | |
1446 | Disc | 10.00 mm | 0.42 mm | 840 | Solid | $12.00 | 11 | |
2473 | Disc | 12.00 mm | 3.00 mm | 840 | Solid | $15.00 | 45 | |
2244 | Disc | 12.70 mm | 0.50 mm | 840 | Solid | $12.00 | 916 | |
2248 | Disc | 12.70 mm | 2.50 mm | 840 | Solid | $12.00 | 17 | |
1454 | Disc | 12.70 mm | 0.85 mm | 840 | Wrap Around | $13.00 | 9 | |
2243 | Disc | 14.00 mm | 0.27 mm | 840 | Solid | $12.00 | 24 | |
2245 | Disc | 14.00 mm | 0.50 mm | 840 | Solid | $12.00 | 12 | |
2249 | Disc | 15.20 mm | 0.50 mm | 840 | Solid | $12.00 | 102 | |
2250 | Disc | 15.30 mm | 0.50 mm | 840 | Solid | $12.00 | 20 | |
2251 | Disc | 15.90 mm | 1.00 mm | 840 | Solid | $12.00 | 105 | |
2242 | Disc | 16.70 mm | 3.00 mm | 840 | Solid | $12.00 | 30 | |
2252 | Disc | 18.50 mm | 3.00 mm | 840 | Solid | $12.00 | 43 | |
2253 | Disc | 19.10 mm | 2.10 mm | 840 | Wrap Around | $15.00 | 16 | |
2247 | Disc | 19.10 mm | 1.00 mm | 840 | Solid | $14.00 | 232 | |
2255 | Disc | 19.80 mm | 2.10 mm | 840 | Solid | $14.00 | 5 | |
2256 | Disc | 19.90 mm | 2.10 mm | 840 | Solid | $14.00 | 25 | |
2267 | Disc | 19.90 mm | 0.53 mm | 840 | Wrap Around | $15.00 | 41 | |
2258 | Disc | 20.00 mm | 2.10 mm | 840 | Solid | $15.00 | 92 | |
2264 | Disc | 20.00 mm | 2.80 mm | 840 | Solid | $15.00 | 27 | |
2259 | Disc | 20.00 mm | 6.00 mm | 840 | Solid | $15.00 | 14 | |
2261 | Disc | 20.00 mm | 10.00 mm | 840 | Solid | $16.00 | 30 | |
2263 | Disc | 20.10 mm | 2.10 mm | 840 | Solid | $15.00 | 60 | |
2262 | Disc | 20.10 mm | 10.00 mm | 840 | Solid | $16.00 | 25 | |
2257 | Disc | 20.20 mm | 2.10 mm | 840 | Solid | $15.00 | 9 | |
2254 | Disc | 20.30 mm | 3.50 mm | 840 | Insulation Band | $16.00 | 17 | |
2260 | Disc | 25.10 mm | 6.40 mm | 840 | Solid | $15.00 | 25 | |
1467 | Disc | 25.30 mm | 2.00 mm | 840 | Solid | $15.00 | 19 | |
1433 | Disc | 25.40 mm | 2.20 mm | 840 | Solid | $15.00 | 95 | |
1458 | Disc | 25.40 mm | 2.20 mm | 840 | Solid | $15.00 | 313 | |
163 | Disc | 30.00 mm | 2.15 mm | 840 | Solid | $15.00 | 11 | |
1472 | Disc | 30.10 mm | 2.10 mm | 840 | Solid | $15.00 | 19 | |
1465 | Disc | 33.30 mm | 2.60 mm | 840 | Solid | $15.00 | 8 | |
2474 | Disc | 35.40 mm | 2.20 mm | 840 | Solid | $21.00 | 15 | |
1466 | Disc | 35.50 mm | 0.39 mm | 840 | Solid | $15.00 | 12 | |
1443 | Disc | 38.00 mm | 3.40 mm | 840 | Insulation Band | $15.00 | 6 | |
2265 | Disc | 50.30 mm | 10.00 mm | 840 | Solid | $20.00 | 5 | |
612 | Disc | 50.60 mm | 2.80 mm | 840 | Insulation Band | $19.00 | 8 | |
2221 | Disc | 9.80 mm | 2.40 mm | 841 | Solid | $12.00 | 11 | |
2465 | Disc | 9.80 mm | 0.80 mm | 841 | Solid | $15.00 | 13 | |
2466 | Disc | 9.90 mm | 0.80 mm | 841 | Solid | $15.00 | 9 | |
2320 | Disc | 9.90 mm | 0.70 mm | 841 | Solid | $12.00 | 150 | |
1562 | Disc | 12.70 mm | 2.60 mm | 841 | Solid | $12.00 | 13 | |
1561 | Disc | 12.80 mm | 2.50 mm | 841 | Solid | $12.00 | 17 | |
2467 | Disc | 16.00 mm | 8.00 mm | 841 | Solid | $16.00 | 26 | |
196 | Disc | 19.00 mm | 2.30 mm | 841 | Solid | $14.00 | 16 | |
2324 | Disc | 19.80 mm | 0.80 mm | 841 | Solid | $14.00 | 19 | |
2323 | Disc | 19.80 mm | 2.20 mm | 841 | Solid | $14.00 | 15 | |
2468 | Disc | 19.90 mm | 0.80 mm | 841 | Solid | $15.00 | 37 | |
2223 | Disc | 20.00 mm | 2.50 mm | 841 | Solid | $15.00 | 5 | |
2325 | Disc | 20.00 mm | 0.80 mm | 841 | Solid | $15.00 | 59 | |
2322 | Disc | 20.10 mm | 4.20 mm | 841 | Solid | $15.00 | 19 | |
2321 | Disc | 20.10 mm | 8.20 mm | 841 | Solid | $15.00 | 10 | |
2469 | Disc | 20.10 mm | 0.80 mm | 841 | Solid | $15.00 | 31 | |
1551 | Disc | 20.10 mm | 0.46 mm | 841 | Wrap Around | $16.00 | 6 | |
764 | Disc | 20.25 mm | 2.30 mm | 841 | Solid | $15.00 | 23 | |
2470 | Disc | 23.00 mm | 2.70 mm | 841 | Solid | $16.00 | 22 | |
1552 | Disc | 24.90 mm | 2.40 mm | 841 | Insulation Band | $15.00 | 23 | |
1550 | Disc | 24.90 mm | 2.40 mm | 841 | Insulation Band | $15.00 | 5 | |
2326 | Disc | 25.00 mm | 0.60 mm | 841 | Solid | $15.00 | 8 | |
2328 | Disc | 25.00 mm | 0.50 mm | 841 | Solid | $15.00 | 20 | |
194 | Disc | 25.00 mm | 0.70 mm | 841 | Solid | $15.00 | 11 | |
2330 | Disc | 25.10 mm | 0.70 mm | 841 | Solid | $15.00 | 10 | |
2329 | Disc | 25.10 mm | 0.50 mm | 841 | Solid | $15.00 | 96 | |
2331 | Disc | 25.20 mm | 0.50 mm | 841 | Solid | $15.00 | 9 | |
2471 | Disc | 25.20 mm | 0.40 mm | 841 | Solid | $15.00 | 17 | |
780 | Disc | 25.40 mm | 0.70 mm | 841 | Solid | $15.00 | 70 | |
2337 | Disc | 30.00 mm | 1.10 mm | 841 | Bullseye | $16.00 | 10 | |
2333 | Disc | 31.90 mm | 1.50 mm | 841 | Solid | $15.00 | 15 | |
2332 | Disc | 31.90 mm | 0.60 mm | 841 | Solid | $15.00 | 16 | |
1555 | Disc | 34.70 mm | 1.30 mm | 841 | Solid | $15.00 | 11 | |
2334 | Disc | 35.20 mm | 0.50 mm | 841 | Solid | $15.00 | 15 | |
2343 | Disc | 37.00 mm | 1.70 mm | 841 | Solid | $15.00 | 13 | |
2335 | Disc | 37.10 mm | 1.30 mm | 841 | Solid | $15.00 | 24 | |
2341 | Disc | 37.80 mm | 1.20 mm | 841 | Insulation Band | $16.00 | 8 | |
2342 | Disc | 37.90 mm | 1.20 mm | 841 | Bullseye | $16.00 | 6 | |
2344 | Disc | 47.90 mm | 1.80 mm | 841 | Solid | $16.00 | 12 | |
2346 | Disc | 48.00 mm | 1.80 mm | 841 | Solid | $16.00 | 10 | |
2345 | Disc | 48.00 mm | 1.70 mm | 841 | Solid | $16.00 | 8 | |
2347 | Disc | 48.10 mm | 1.40 mm | 841 | Solid | $16.00 | 6 | |
1119 | Disc | 5.00 mm | 0.50 mm | 842 | Solid | $12.00 | 16 | |
801 | Disc | 6.40 mm | 1.90 mm | 842 | Solid | $12.00 | 188 | |
800 | Disc | 6.50 mm | 1.00 mm | 842 | Solid | $12.00 | 233 | |
799 | Disc | 9.30 mm | 2.10 mm | 842 | Solid | $12.00 | 107 | |
1116 | Disc | 9.90 mm | 1.00 mm | 842 | Solid | $12.00 | 42 | |
1113 | Disc | 10.00 mm | 1.20 mm | 842 | Solid | $12.00 | 15 | |
1096 | Disc | 12.60 mm | 1.30 mm | 842 | Solid | $12.00 | 20 | |
1114 | Disc | 12.60 mm | 1.00 mm | 842 | Solid | $12.00 | 24 | |
874 | Disc | 15.20 mm | 0.50 mm | 842 | Solid | $12.00 | 25 | |
794 | Disc | 15.80 mm | 3.00 mm | 842 | Solid | $12.00 | 9 | |
797 | Disc | 18.40 mm | 3.00 mm | 842 | Solid | $12.00 | 85 | |
1106 | Disc | 18.50 mm | 3.00 mm | 842 | Solid | $12.00 | 7 | |
795 | Disc | 19.10 mm | 2.10 mm | 842 | Solid | $14.00 | 156 | |
820 | Disc | 25.50 mm | 4.30 mm | 842 | Solid | $15.00 | 15 | |
817 | Disc | 25.60 mm | 4.30 mm | 842 | Solid | $15.00 | 43 | |
819 | Disc | 25.70 mm | 4.30 mm | 842 | Solid | $15.00 | 5 | |
257 | Disc | 50.80 mm | 2.55 mm | 842 | Solid | $19.00 | 274 | |
543 | Disc | 50.80 mm | 2.65 mm | 842 | Insulation Band | $19.00 | 5 | |
1791 | Disc | 4.00 mm | 2.00 mm | 844 | Solid | $12.00 | 117 | |
1776 | Disc | 9.90 mm | 10.00 mm | 844 | Solid | $15.00 | 6 | |
1790 | Disc | 12.70 mm | 2.50 mm | 844 | Solid | $12.00 | 9 | |
1777 | Disc | 12.80 mm | 1.00 mm | 844 | Solid | $12.00 | 28 | |
790 | Disc | 19.80 mm | 0.80 mm | 844 | Insulation Band | $14.00 | 565 | |
1757 | Disc | 29.90 mm | 2.00 mm | 844 | Solid | $15.00 | 16 | |
1761 | Disc | 30.00 mm | 2.00 mm | 844 | Solid | $15.00 | 19 | |
580 | Disc | 4.50 mm | 0.77 mm | 850 | Solid | $12.00 | 215 | |
955 | Disc | 4.70 mm | 0.60 mm | 850 | Solid | $12.00 | 280 | |
975 | Disc | 4.70 mm | 3.40 mm | 850 | Solid | $12.00 | 54 | |
970 | Disc | 4.70 mm | 0.80 mm | 850 | Solid | $12.00 | 264 | |
948 | Disc | 4.70 mm | 0.46 mm | 850 | Solid | $12.00 | 156 | |
963 | Disc | 4.80 mm | 0.68 mm | 850 | Solid | $12.00 | 844 | |
581 | Disc | 4.90 mm | 0.75 mm | 850 | Solid | $12.00 | 186 | |
958 | Disc | 4.90 mm | 0.90 mm | 850 | Solid | $12.00 | 5 | |
1129 | Disc | 4.90 mm | 1.00 mm | 850 | Solid | $12.00 | 73 | |
966 | Disc | 4.90 mm | 0.42 mm | 850 | Solid | $12.00 | 558 | |
978 | Disc | 5.00 mm | 0.70 mm | 850 | Solid | $12.00 | 232 | |
1339 | Disc | 5.10 mm | 1.50 mm | 850 | Solid | $12.00 | 358 | |
431 | Disc | 6.40 mm | 0.26 mm | 850 | Solid | $12.00 | 5 | |
968 | Disc | 6.40 mm | 0.40 mm | 850 | Solid | $12.00 | 5 | |
435 | Disc | 8.00 mm | 0.40 mm | 850 | Solid | $12.00 | 104 | |
1337 | Disc | 8.10 mm | 8.30 mm | 850 | Solid | $12.00 | 67 | |
1340 | Disc | 8.30 mm | 0.64 mm | 850 | Solid | $12.00 | 146 | |
976 | Disc | 8.80 mm | 3.00 mm | 850 | Solid | $12.00 | 155 | |
937 | Disc | 8.90 mm | 3.00 mm | 850 | Tab | $13.00 | 317 | |
1335 | Disc | 8.90 mm | 7.90 mm | 850 | Tab | $13.00 | 121 | |
1344 | Disc | 9.50 mm | 1.00 mm | 850 | Solid | $12.00 | 1841 | |
443 | Disc | 9.50 mm | 1.80 mm | 850 | Solid | $12.00 | 7 | |
760 | Disc | 9.50 mm | 3.90 mm | 850 | Tab | $13.00 | 47 | |
63 | Disc | 9.50 mm | 1.00 mm | 850 | Wrap Around | $13.00 | 721 | |
1350 | Disc | 9.50 mm | 3.40 mm | 850 | Tab | $13.00 | 518 | |
1349 | Disc | 9.50 mm | 3.40 mm | 850 | Tab | $13.00 | 76 | |
1853 | Disc | 9.60 mm | 1.00 mm | 850 | Wrap Around | $13.00 | 68 | |
1125 | Disc | 10.00 mm | 0.52 mm | 850 | Solid | $12.00 | 126 | |
1103 | Disc | 10.00 mm | 0.48 mm | 850 | Solid | $12.00 | 12 | |
2209 | Disc | 10.00 mm | 2.10 mm | 850 | Solid | $12.00 | 39 | |
1336 | Disc | 10.00 mm | 10.00 mm | 850 | Solid | $15.00 | 37 | |
1346 | Disc | 10.00 mm | 1.40 mm | 850 | Solid | $12.00 | 13 | |
406 | Disc | 10.00 mm | 0.50 mm | 850 | Solid | $12.00 | 10 | |
407 | Disc | 10.00 mm | 1.85 mm | 850 | Solid | $12.00 | 363 | |
1127 | Disc | 10.10 mm | 0.50 mm | 850 | Solid | $12.00 | 107 | |
972 | Disc | 10.10 mm | 1.80 mm | 850 | Solid | $12.00 | 122 | |
408 | Disc | 10.15 mm | 6.40 mm | 850 | Solid | $12.00 | 198 | |
960 | Disc | 10.20 mm | 1.40 mm | 850 | Solid | $12.00 | 521 | |
410 | Disc | 10.20 mm | 6.40 mm | 850 | Solid | $12.00 | 45 | |
411 | Disc | 10.30 mm | 1.40 mm | 850 | Solid | $12.00 | 612 | |
472 | Disc | 11.40 mm | 10.60 mm | 850 | Solid | $15.00 | 735 | |
2210 | Disc | 11.90 mm | 0.70 mm | 850 | Wrap Around | $13.00 | 2944 | |
448 | Disc | 12.00 mm | 0.50 mm | 850 | Solid | $12.00 | 28 | |
2230 | Disc | 12.50 mm | 2.10 mm | 850 | Solid | $12.00 | 155 | |
1343 | Disc | 12.60 mm | 6.50 mm | 850 | Solid | $12.00 | 30 | |
588 | Disc | 12.50 mm | 2.00 mm | 850 | Solid | $12.00 | 342 | |
964 | Disc | 12.60 mm | 2.00 mm | 850 | Solid | $12.00 | 11 | |
2201 | Disc | 12.60 mm | 1.00 mm | 850 | Solid | $12.00 | 911 | |
401 | Disc | 12.60 mm | 0.50 mm | 850 | Solid | $12.00 | 11 | |
599 | Disc | 12.60 mm | 3.20 mm | 850 | Solid | $12.00 | 158 | |
590 | Disc | 12.70 mm | 1.60 mm | 850 | Solid | $12.00 | 296 | |
591 | Disc | 12.70 mm | 0.50 mm | 850 | Solid | $12.00 | 188 | |
1907 | Disc | 12.70 mm | 1.00 mm | 850 | Solid | $12.00 | 2672 | |
1299 | Disc | 12.70 mm | 0.50 mm | 850 | Wrap Around | $13.00 | 30 | |
589 | Disc | 12.70 mm | 3.30 mm | 850 | Solid | $12.00 | 252 | |
1307 | Disc | 12.70 mm | 2.20 mm | 850 | Wrap Around | $13.00 | 6 | |
592 | Disc | 12.72 mm | 2.03 mm | 850 | Solid | $12.00 | 405 | |
397 | Disc | 12.75 mm | 2.00 mm | 850 | Solid | $12.00 | 281 | |
1288 | Disc | 12.80 mm | 2.00 mm | 850 | Solid | $12.00 | 91 | |
1282 | Disc | 12.90 mm | 2.00 mm | 850 | Wrap Around | $13.00 | 161 | |
595 | Disc | 12.90 mm | 2.10 mm | 850 | Solid | $12.00 | 30 | |
1289 | Disc | 12.90 mm | 2.00 mm | 850 | Solid | $12.00 | 30 | |
994 | Disc | 13.00 mm | 2.00 mm | 850 | Solid | $12.00 | 369 | |
1009 | Disc | 13.10 mm | 2.00 mm | 850 | Solid | $12.00 | 223 | |
999 | Disc | 13.60 mm | 2.00 mm | 850 | Solid | $12.00 | 9 | |
2215 | Disc | 14.00 mm | 12.00 mm | 850 | Solid | $14.00 | 83 | |
989 | Disc | 14.60 mm | 2.00 mm | 850 | Solid | $12.00 | 416 | |
2213 | Disc | 14.80 mm | 1.50 mm | 850 | Solid | $12.00 | 34 | |
991 | Disc | 15.80 mm | 0.80 mm | 850 | Solid | $12.00 | 11 | |
993 | Disc | 15.90 mm | 1.80 mm | 850 | Solid | $12.00 | 121 | |
1007 | Disc | 15.90 mm | 2.00 mm | 850 | Solid | $12.00 | 254 | |
2216 | Disc | 16.00 mm | 2.10 mm | 850 | Solid | $12.00 | 37 | |
1345 | Disc | 16.80 mm | 0.25 mm | 850 | Solid | $12.00 | 164 | |
1331 | Disc | 16.90 mm | 0.28 mm | 850 | Solid | $12.00 | 439 | |
1005 | Disc | 18.00 mm | 1.70 mm | 850 | Solid | $12.00 | 15 | |
2217 | Disc | 18.00 mm | 2.10 mm | 850 | Solid | $12.00 | 100 | |
2218 | Disc | 18.00 mm | 5.00 mm | 850 | Solid | $12.00 | 9 | |
2188 | Disc | 19.00 mm | 12.10 mm | 850 | Solid | $20.00 | 28 | |
1537 | Disc | 19.00 mm | 2.10 mm | 850 | Solid | $14.00 | 76 | |
2203 | Disc | 19.00 mm | 12.00 mm | 850 | Solid | $14.00 | 10 | |
988 | Disc | 19.00 mm | 12.00 mm | 850 | Solid | $20.00 | 56 | |
454 | Disc | 19.00 mm | 1.00 mm | 850 | Solid | $14.00 | 308 | |
944 | Disc | 19.00 mm | 1.00 mm | 850 | Wrap Around | $15.00 | 6 | |
1544 | Disc | 19.10 mm | 2.10 mm | 850 | Solid | $14.00 | 16 | |
787 | Disc | 19.10 mm | 6.10 mm | 850 | Solid | $14.00 | 29 | |
1341 | Disc | 19.80 mm | 0.70 mm | 850 | Solid | $14.00 | 40 | |
1542 | Disc | 19.80 mm | 1.40 mm | 850 | Solid | $14.00 | 10 | |
1531 | Disc | 19.90 mm | 0.43 mm | 850 | Solid | $14.00 | 43 | |
1545 | Disc | 19.90 mm | 0.80 mm | 850 | Solid | $14.00 | 92 | |
1548 | Disc | 19.90 mm | 2.80 mm | 850 | Solid | $14.00 | 56 | |
1539 | Disc | 19.90 mm | 2.10 mm | 850 | Solid | $15.00 | 36 | |
1027 | Disc | 19.90 mm | 1.00 mm | 850 | Solid | $14.00 | 31 | |
2219 | Disc | 20.00 mm | 1.20 mm | 850 | Wrap Around | $16.00 | 12 | |
1892 | Disc | 23.10 mm | 2.00 mm | 850 | Solid | $15.00 | 359 | |
936 | Disc | 25.10 mm | 1.60 mm | 850 | Solid | $15.00 | 291 | |
1314 | Disc | 25.20 mm | 1.00 mm | 850 | Wrap Around | $16.00 | 16 | |
1543 | Disc | 25.20 mm | 1.80 mm | 850 | Solid | $15.00 | 14 | |
385 | Disc | 25.35 mm | 2.05 mm | 850 | Wrap Around | $16.00 | 627 | |
1546 | Disc | 25.40 mm | 1.80 mm | 850 | Solid | $15.00 | 22 | |
474 | Disc | 25.40 mm | 2.00 mm | 850 | Wrap Around | $14.00 | 6 | |
344 | Disc | 25.40 mm | 0.50 mm | 850 | Wrap Around | $16.00 | 628 | |
1536 | Disc | 25.40 mm | 2.10 mm | 850 | Solid | $15.00 | 8 | |
1077 | Disc | 25.50 mm | 1.60 mm | 850 | Solid | $15.00 | 75 | |
1011 | Disc | 26.00 mm | 4.60 mm | 850 | Solid | $15.00 | 199 | |
1024 | Disc | 26.10 mm | 4.60 mm | 850 | Solid | $15.00 | 30 | |
1533 | Disc | 28.50 mm | 4.00 mm | 850 | Solid | $15.00 | 214 | |
1518 | Disc | 30.00 mm | 0.52 mm | 850 | Wrap Around | $16.00 | 92 | |
1517 | Disc | 30.10 mm | 0.52 mm | 850 | Wrap Around | $16.00 | 25 | |
1013 | Disc | 31.60 mm | 2.70 mm | 850 | Solid | $15.00 | 47 | |
1525 | Disc | 37.80 mm | 0.90 mm | 850 | Solid | $15.00 | 15 | |
1315 | Disc | 38.10 mm | 4.10 mm | 850 | Wrap Around | $16.00 | 18 | |
1310 | Disc | 38.10 mm | 4.00 mm | 850 | Wrap Around | $16.00 | 12 | |
1192 | Disc | 3.90 mm | 0.50 mm | 851 | Solid | $12.00 | 231 | |
1201 | Disc | 4.70 mm | 3.40 mm | 851 | Solid | $12.00 | 71 | |
1204 | Disc | 4.80 mm | 0.80 mm | 851 | Solid | $12.00 | 2200 | |
1266 | Disc | 5.00 mm | 1.00 mm | 851 | Solid | $12.00 | 19 | |
1265 | Disc | 5.00 mm | 0.50 mm | 851 | Solid | $12.00 | 29 | |
1264 | Disc | 5.00 mm | 0.30 mm | 851 | Solid | $12.00 | 12 | |
1257 | Disc | 5.80 mm | 0.20 mm | 851 | Solid | $12.00 | 5 | |
1256 | Disc | 6.00 mm | 0.39 mm | 851 | Solid | $12.00 | 66 | |
1259 | Disc | 6.00 mm | 1.00 mm | 851 | Solid | $12.00 | 29 | |
1258 | Disc | 6.00 mm | 0.20 mm | 851 | Solid | $12.00 | 5 | |
1239 | Disc | 6.20 mm | 0.25 mm | 851 | Solid | $12.00 | 35 | |
1236 | Disc | 6.30 mm | 0.40 mm | 851 | Solid | $12.00 | 18 | |
43 | Disc | 6.35 mm | 0.76 mm | 851 | Solid | $12.00 | 13 | |
850 | Disc | 6.50 mm | 0.27 mm | 851 | Wrap Around | $13.00 | 930 | |
1235 | Disc | 6.90 mm | 0.20 mm | 851 | Solid | $12.00 | 25 | |
1238 | Disc | 7.00 mm | 0.25 mm | 851 | Solid | $12.00 | 21 | |
20 | Disc | 7.66 mm | 2.05 mm | 851 | Solid | $12.00 | 83 | |
1260 | Disc | 7.80 mm | 0.70 mm | 851 | Solid | $12.00 | 124 | |
1252 | Disc | 8.60 mm | 0.60 mm | 851 | Solid | $12.00 | 48 | |
758 | Disc | 9.00 mm | 3.00 mm | 851 | Tab | $13.00 | 38 | |
42 | Disc | 9.35 mm | 2.05 mm | 851 | Solid | $12.00 | 68 | |
1249 | Disc | 9.50 mm | 2.00 mm | 851 | Solid | $12.00 | 15 | |
1247 | Disc | 9.50 mm | 0.50 mm | 851 | Solid | $12.00 | 5 | |
1248 | Disc | 9.50 mm | 1.00 mm | 851 | Solid | $12.00 | 16 | |
1193 | Disc | 9.80 mm | 2.10 mm | 851 | Solid | $12.00 | 263 | |
1227 | Disc | 9.90 mm | 1.00 mm | 851 | Solid | $12.00 | 148 | |
1226 | Disc | 10.00 mm | 3.00 mm | 851 | Solid | $12.00 | 8 | |
957 | Disc | 10.00 mm | 2.00 mm | 851 | Solid | $12.00 | 429 | |
1233 | Disc | 10.00 mm | 0.50 mm | 851 | Solid | $12.00 | 20 | |
1243 | Disc | 10.00 mm | 1.40 mm | 851 | Solid | $12.00 | 29 | |
1194 | Disc | 10.00 mm | 0.72 mm | 851 | Solid | $12.00 | 2581 | |
18 | Disc | 10.00 mm | 1.00 mm | 851 | Solid | $12.00 | 452 | |
1199 | Disc | 10.10 mm | 1.40 mm | 851 | Solid | $12.00 | 5 | |
1232 | Disc | 10.10 mm | 0.50 mm | 851 | Solid | $12.00 | 40 | |
1241 | Disc | 10.10 mm | 2.04 mm | 851 | Solid | $12.00 | 83 | |
1198 | Disc | 10.10 mm | 1.85 mm | 851 | Solid | $12.00 | 8 | |
1130 | Disc | 10.10 mm | 1.00 mm | 851 | Solid | $12.00 | 116 | |
1242 | Disc | 10.20 mm | 2.00 mm | 851 | Solid | $12.00 | 22 | |
1255 | Disc | 11.90 mm | 0.84 mm | 851 | Solid | $12.00 | 30 | |
1254 | Disc | 11.90 mm | 0.50 mm | 851 | Solid | $12.00 | 9 | |
1229 | Disc | 11.90 mm | 2.00 mm | 851 | Solid | $12.00 | 14 | |
1196 | Disc | 12.00 mm | 1.80 mm | 851 | Solid | $12.00 | 320 | |
1162 | Disc | 14.00 mm | 2.10 mm | 851 | Solid | $12.00 | 40 | |
1172 | Disc | 12.00 mm | 2.10 mm | 851 | Solid | $12.00 | 348 | |
1188 | Disc | 12.70 mm | 3.20 mm | 851 | Solid | $12.00 | 80 | |
1231 | Disc | 12.80 mm | 4.30 mm | 851 | Solid | $12.00 | 379 | |
1189 | Disc | 12.90 mm | 0.53 mm | 851 | Solid | $12.00 | 6 | |
1246 | Disc | 13.00 mm | 2.00 mm | 851 | Solid | $12.00 | 12 | |
1245 | Disc | 15.00 mm | 0.70 mm | 851 | Solid | $12.00 | 18 | |
1171 | Disc | 15.80 mm | 3.20 mm | 851 | Solid | $12.00 | 13 | |
1163 | Disc | 15.85 mm | 2.00 mm | 851 | Solid | $12.00 | 23 | |
1160 | Disc | 17.90 mm | 1.70 mm | 851 | Solid | $12.00 | 21 | |
1224 | Disc | 18.00 mm | 1.20 mm | 851 | Solid | $12.00 | 27 | |
1200 | Disc | 18.00 mm | 2.10 mm | 851 | Solid | $12.00 | 96 | |
1244 | Disc | 19.00 mm | 1.00 mm | 851 | Solid | $14.00 | 10 | |
1195 | Disc | 19.05 mm | 1.00 mm | 851 | Solid | $14.00 | 252 | |
1157 | Disc | 19.10 mm | 2.00 mm | 851 | Solid | $14.00 | 130 | |
1158 | Disc | 19.20 mm | 2.00 mm | 851 | Solid | $14.00 | 38 | |
1169 | Disc | 19.90 mm | 0.75 mm | 851 | Solid | $14.00 | 65 | |
1049 | Disc | 20.00 mm | 1.80 mm | 851 | Insulation Band | $15.00 | 119 | |
1173 | Disc | 20.00 mm | 1.00 mm | 851 | Solid | $15.00 | 74 | |
1156 | Disc | 25.10 mm | 1.00 mm | 851 | Solid | $15.00 | 241 | |
1184 | Disc | 25.20 mm | 2.50 mm | 851 | Solid | $15.00 | 26 | |
1170 | Disc | 25.20 mm | 2.00 mm | 851 | Solid | $15.00 | 51 | |
1165 | Disc | 25.30 mm | 1.00 mm | 851 | Solid | $15.00 | 63 | |
1039 | Disc | 25.30 mm | 2.10 mm | 851 | Wrap Around | $16.00 | 15 | |
1038 | Disc | 25.30 mm | 2.10 mm | 851 | Solid | $15.00 | 290 | |
1202 | Disc | 25.40 mm | 2.10 mm | 851 | Solid | $15.00 | 121 | |
1140 | Disc | 25.40 mm | 0.50 mm | 851 | Solid | $15.00 | 74 | |
1174 | Disc | 25.40 mm | 1.80 mm | 851 | Solid | $15.00 | 109 | |
1284 | Disc | 25.50 mm | 2.50 mm | 851 | Solid | $15.00 | 29 | |
2386 | Disc | 3.20 mm | 1.00 mm | 855 | Solid | $12.00 | 43 | |
1945 | Disc | 6.20 mm | 1.00 mm | 855 | Solid | $12.00 | 21 | |
1870 | Disc | 6.20 mm | 4.00 mm | 855 | Solid | $12.00 | 32 | |
1869 | Disc | 6.40 mm | 8.00 mm | 855 | Solid | $12.00 | 11 | |
2387 | Disc | 6.40 mm | 3.80 mm | 855 | Solid | $12.00 | 36 | |
1946 | Disc | 6.40 mm | 1.00 mm | 855 | Solid | $12.00 | 21 | |
1947 | Disc | 6.50 mm | 2.00 mm | 855 | Solid | $12.00 | 30 | |
1995 | Disc | 6.50 mm | 1.00 mm | 855 | Solid | $12.00 | 77 | |
1948 | Disc | 7.60 mm | 2.50 mm | 855 | Solid | $12.00 | 24 | |
2388 | Disc | 7.80 mm | 3.00 mm | 855 | Solid | $12.00 | 20 | |
2389 | Disc | 8.00 mm | 3.00 mm | 855 | Solid | $12.00 | 13 | |
1871 | Disc | 9.00 mm | 6.00 mm | 855 | Solid | $12.00 | 31 | |
2240 | Disc | 9.70 mm | 0.26 mm | 855 | Other | $13.00 | 25 | |
1942 | Disc | 9.90 mm | 1.00 mm | 855 | Solid | $12.00 | 18 | |
1906 | Disc | 12.00 mm | 2.10 mm | 855 | Solid | $12.00 | 111 | |
1880 | Disc | 12.50 mm | 2.10 mm | 855 | Solid | $12.00 | 33 | |
1877 | Disc | 12.60 mm | 2.10 mm | 855 | Solid | $12.00 | 31 | |
1100 | Disc | 12.70 mm | 8.00 mm | 855 | Solid | $15.00 | 18 | |
1911 | Disc | 12.70 mm | 3.50 mm | 855 | Solid | $12.00 | 22 | |
1900 | Disc | 12.70 mm | 0.28 mm | 855 | Solid | $12.00 | 9 | |
1960 | Disc | 12.70 mm | 0.52 mm | 855 | Solid | $12.00 | 51 | |
1899 | Disc | 12.70 mm | 2.00 mm | 855 | Solid | $12.00 | 49 | |
1962 | Disc | 12.80 mm | 1.00 mm | 855 | Solid | $12.00 | 17 | |
1901 | Disc | 12.80 mm | 0.28 mm | 855 | Solid | $12.00 | 7 | |
2391 | Disc | 12.80 mm | 2.00 mm | 855 | Solid | $12.00 | 5 | |
2392 | Disc | 12.90 mm | 2.00 mm | 855 | Solid | $12.00 | 11 | |
1872 | Disc | 12.90 mm | 9.10 mm | 855 | Solid | $12.00 | 13 | |
1873 | Disc | 13.00 mm | 8.70 mm | 855 | Solid | $12.00 | 83 | |
1963 | Disc | 13.40 mm | 0.40 mm | 855 | Solid | $12.00 | 7 | |
1881 | Disc | 13.80 mm | 2.00 mm | 855 | Solid | $12.00 | 15 | |
1878 | Disc | 13.90 mm | 2.00 mm | 855 | Solid | $12.00 | 20 | |
1884 | Disc | 16.00 mm | 2.70 mm | 855 | Solid | $12.00 | 56 | |
1882 | Disc | 16.00 mm | 2.70 mm | 855 | Solid | $12.00 | 12 | |
1876 | Disc | 16.00 mm | 1.00 mm | 855 | Solid | $12.00 | 5 | |
1908 | Disc | 19.00 mm | 2.00 mm | 855 | Solid | $12.00 | 11 | |
1865 | Disc | 19.00 mm | 9.70 mm | 855 | Solid | $14.00 | 5 | |
1867 | Disc | 19.10 mm | 9.40 mm | 855 | Solid | $14.00 | 8 | |
1905 | Disc | 19.10 mm | 1.00 mm | 855 | Solid | $12.00 | 13 | |
1862 | Disc | 19.10 mm | 9.70 mm | 855 | Solid | $14.00 | 13 | |
1883 | Disc | 19.90 mm | 2.00 mm | 855 | Solid | $14.00 | 9 | |
2394 | Disc | 20.00 mm | 2.00 mm | 855 | Solid | $15.00 | 5 | |
2395 | Disc | 20.00 mm | 12.10 mm | 855 | Solid | $16.00 | 9 | |
2396 | Disc | 20.10 mm | 12.10 mm | 855 | Solid | $16.00 | 6 | |
1953 | Disc | 25.00 mm | 0.51 mm | 855 | Solid | $15.00 | 5 | |
2398 | Disc | 25.00 mm | 6.30 mm | 855 | Tab | $15.00 | 5 | |
2399 | Disc | 25.10 mm | 6.30 mm | 855 | Solid | $15.00 | 14 | |
1951 | Disc | 25.30 mm | 0.27 mm | 855 | Solid | $15.00 | 5 | |
1904 | Disc | 25.30 mm | 0.27 mm | 855 | Solid | $15.00 | 6 | |
1895 | Disc | 25.30 mm | 6.30 mm | 855 | Tab | $17.00 | 6 | |
1912 | Disc | 25.40 mm | 2.00 mm | 855 | Solid | $15.00 | 11 | |
1896 | Disc | 25.40 mm | 6.30 mm | 855 | Tab | $17.00 | 49 | |
2400 | Disc | 25.50 mm | 6.30 mm | 855 | Solid | $22.00 | 14 | |
2487 | Disc | 25.60 mm | 6.40 mm | 855 | Solid | $22.00 | 18 | |
2486 | Disc | 25.60 mm | 6.30 mm | 855 | Tab | $22.00 | 10 | |
2488 | Disc | 25.70 mm | 6.30 mm | 855 | Solid | $22.00 | 6 | |
1954 | Disc | 29.90 mm | 0.27 mm | 855 | Solid | $15.00 | 5 | |
1893 | Disc | 30.00 mm | 0.52 mm | 855 | Wrap Around | $16.00 | 35 | |
1885 | Disc | 34.10 mm | 0.25 mm | 855 | Solid | $15.00 | 25 | |
2500 | Disc | 4.00 mm | 0.50 mm | 880 | Solid | $15.00 | 55 | |
2007 | Disc | 4.90 mm | 0.60 mm | 880 | Solid | $12.00 | 69 | |
1334 | Disc | 5.10 mm | 0.40 mm | 880 | Solid | $12.00 | 784 | |
2008 | Disc | 5.90 mm | 2.90 mm | 880 | Solid | $12.00 | 46 | |
2009 | Disc | 7.50 mm | 0.27 mm | 880 | Solid | $12.00 | 22 | |
2501 | Disc | 7.80 mm | 0.50 mm | 880 | Wrap Around | $15.00 | 19 | |
1131 | Disc | 9.10 mm | 1.40 mm | 880 | Wrap Around | $13.00 | 18 | |
2456 | Disc | 9.50 mm | 0.30 mm | 880 | Solid | $15.00 | 54 | |
2081 | Disc | 10.00 mm | 10.00 mm | 880 | Solid | $15.00 | 7 | |
2080 | Disc | 10.00 mm | 1.00 mm | 880 | Solid | $12.00 | 27 | |
2079 | Disc | 10.00 mm | 0.80 mm | 880 | Solid | $12.00 | 14 | |
1153 | Disc | 11.10 mm | 2.30 mm | 880 | Solid | $12.00 | 207 | |
1138 | Disc | 11.20 mm | 2.30 mm | 880 | Solid | $12.00 | 783 | |
2083 | Disc | 11.30 mm | 2.30 mm | 880 | Solid | $12.00 | 18 | |
2006 | Disc | 14.90 mm | 0.53 mm | 880 | Solid | $12.00 | 9 | |
2457 | Disc | 14.90 mm | 1.30 mm | 880 | Solid | $15.00 | 9 | |
1151 | Disc | 15.00 mm | 2.10 mm | 880 | Solid | $12.00 | 41 | |
2459 | Disc | 15.10 mm | 1.30 mm | 880 | Solid | $15.00 | 8 | |
2458 | Disc | 15.00 mm | 1.30 mm | 880 | Solid | $15.00 | 10 | |
2084 | Disc | 15.90 mm | 6.40 mm | 880 | Solid | $12.00 | 21 | |
2460 | Disc | 18.00 mm | 1.50 mm | 880 | Solid | $15.00 | 7 | |
2433 | Disc | 19.90 mm | 9.90 mm | 2.50 mm | 880 | Solid | $18.00 | 20 |
2085 | Disc | 19.00 mm | 2.10 mm | 880 | Solid | $14.00 | 45 | |
2086 | Disc | 19.00 mm | 8.40 mm | 880 | Solid | $14.00 | 36 | |
2461 | Disc | 19.10 mm | 4.10 mm | 880 | Solid | $16.00 | 32 | |
2087 | Disc | 19.10 mm | 3.20 mm | 880 | Solid | $14.00 | 236 | |
1333 | Disc | 19.00 mm | 4.10 mm | 880 | Solid | $14.00 | 65 | |
2088 | Disc | 19.80 mm | 1.00 mm | 880 | Solid | $14.00 | 34 | |
2089 | Disc | 20.00 mm | 2.00 mm | 880 | Solid | $15.00 | 12 | |
2090 | Disc | 22.20 mm | 1.20 mm | 880 | Solid | $15.00 | 15 | |
2091 | Disc | 22.30 mm | 1.20 mm | 880 | Solid | $15.00 | 19 | |
2092 | Disc | 22.40 mm | 1.20 mm | 880 | Solid | $15.00 | 5 | |
2093 | Disc | 24.00 mm | 3.00 mm | 880 | Solid | $15.00 | 14 | |
2224 | Disc | 24.80 mm | 0.70 mm | 880 | Solid | $15.00 | 25 | |
2094 | Disc | 24.90 mm | 0.70 mm | 880 | Solid | $15.00 | 10 | |
1149 | Disc | 25.00 mm | 2.10 mm | 880 | Solid | $15.00 | 64 | |
2003 | Disc | 25.40 mm | 0.44 mm | 880 | Solid | $15.00 | 5 | |
2097 | Disc | 25.40 mm | 1.00 mm | 880 | Solid | $15.00 | 10 | |
2102 | Disc | 29.90 mm | 2.30 mm | 880 | Solid | $15.00 | 12 | |
2103 | Disc | 30.00 mm | 2.30 mm | 880 | Solid | $15.00 | 21 | |
2104 | Disc | 30.10 mm | 2.30 mm | 880 | Solid | $15.00 | 14 | |
2105 | Disc | 32.20 mm | 2.30 mm | 880 | Solid | $15.00 | 8 | |
2106 | Disc | 30.30 mm | 2.30 mm | 880 | Solid | $15.00 | 7 | |
2108 | Disc | 34.90 mm | 0.43 mm | 880 | Solid | $15.00 | 9 | |
1146 | Disc | 10.00 mm | 0.50 mm | 881 | Solid | $12.00 | 12 | |
1142 | Disc | 12.50 mm | 0.50 mm | 881 | Solid | $12.00 | 44 | |
1268 | Disc | 18.90 mm | 3.20 mm | 881 | Solid | $12.00 | 111 | |
2485 | Disc | 30.00 mm | 2.10 mm | 881 | Insulation Band | $21.00 | 24 | |
1274 | Disc | 14.70 mm | 2.10 mm | Type II | Solid | $12.00 | 300 | |
2497 | Disc | 9.60 mm | 1.00 mm | Type I | Solid | $15.00 | 188 | |
2204 | Disc | 50.60 mm | 2.80 mm | Type I | Insulation Band | $19.00 | 8 | |
1273 | Disc | 14.50 mm | 1.90 mm | Type II | Solid | $12.00 | 496 | |
1400 | Disc | 22.70 mm | 0.16 mm | Type VI | Insulation Band | $5.00 | 10065 | |
1686 | Plate | 2.00 mm | 2.00 mm | 4.00 mm | 840 | Solid | $12.00 | 21 |
1685 | Plate | 2.00 mm | 2.00 mm | 9.00 mm | 840 | Solid | $12.00 | 5 |
1673 | Plate | 2.50 mm | 2.50 mm | 6.00 mm | 840 | Solid | $12.00 | 129 |
2338 | Plate | 2.50 mm | 2.50 mm | 2.40 mm | 840 | Solid | $12.00 | 130 |
1682 | Plate | 4.50 mm | 2.00 mm | 0.52 mm | 840 | Wrap Around | $13.00 | 77 |
2277 | Plate | 5.00 mm | 2.50 mm | 0.35 mm | 840 | Solid | $12.00 | 231 |
2274 | Plate | 5.00 mm | 5.00 mm | 0.51 mm | 840 | Solid | $12.00 | 49 |
1683 | Plate | 5.00 mm | 3.10 mm | 3.00 mm | 840 | Solid | $12.00 | 90 |
1394 | Plate | 5.00 mm | 5.00 mm | 2.00 mm | 840 | Solid | $12.00 | 526 |
268 | Plate | 6.35 mm | 6.35 mm | 0.75 mm | 840 | Solid | $12.00 | 189 |
1670 | Plate | 6.40 mm | 4.40 mm | 1.00 mm | 840 | Solid | $12.00 | 295 |
1703 | Plate | 7.70 mm | 6.40 mm | 3.90 mm | 840 | Solid | $12.00 | 43 |
260 | Plate | 10.00 mm | 10.00 mm | 0.50 mm | 840 | Solid | $12.00 | 20 |
1679 | Plate | 10.50 mm | 3.00 mm | 4.10 mm | 840 | Solid | $12.00 | 21 |
1676 | Plate | 10.50 mm | 3.00 mm | 4.30 mm | 840 | Solid | $12.00 | 159 |
1480 | Plate | 10.50 mm | 3.00 mm | 4.30 mm | 840 | Solid | $12.00 | 220 |
1677 | Plate | 10.50 mm | 3.00 mm | 3.90 mm | 840 | Solid | $12.00 | 14 |
1403 | Plate | 11.00 mm | 10.00 mm | 1.50 mm | 840 | Insulation Band | $12.00 | 49 |
1655 | Plate | 12.90 mm | 10.60 mm | 0.52 mm | 840 | Bullseye | $12.00 | 9 |
2279 | Plate | 13.00 mm | 1.00 mm | 1.10 mm | 840 | Wrap Around | $13.00 | 22 |
240 | Plate | 14.50 mm | 12.00 mm | 2.20 mm | 840 | Solid | $12.00 | 60 |
1684 | Plate | 15.10 mm | 5.00 mm | 2.10 mm | 840 | Solid | $12.00 | 27 |
2278 | Plate | 15.50 mm | 5.00 mm | 2.00 mm | 840 | Solid | $12.00 | 67 |
1388 | Plate | 15.90 mm | 5.10 mm | 0.26 mm | 840 | Solid | $12.00 | 40 |
1389 | Plate | 16.10 mm | 5.00 mm | 0.28 mm | 840 | Solid | $12.00 | 26 |
1395 | Plate | 17.00 mm | 2.40 mm | 3.80 mm | 840 | Solid | $12.00 | 135 |
2276 | Plate | 20.00 mm | 15.00 mm | 1.70 mm | 840 | Solid | $15.00 | 8 |
2275 | Plate | 20.00 mm | 15.00 mm | 0.52 mm | 840 | Solid | $15.00 | 32 |
1666 | Plate | 21.00 mm | 2.00 mm | 0.80 mm | 840 | Solid | $15.00 | 9 |
1667 | Plate | 21.00 mm | 8.20 mm | 0.53 mm | 840 | Solid | $15.00 | 40 |
2283 | Plate | 22.50 mm | 9.00 mm | 0.90 mm | 840 | Solid | $15.00 | 26 |
2280 | Plate | 25.00 mm | 25.00 mm | 1.40 mm | 840 | Solid | $25.00 | 8 |
2281 | Plate | 25.20 mm | 25.20 mm | 0.50 mm | 840 | Solid | $25.00 | 7 |
1701 | Plate | 25.40 mm | 25.40 mm | 0.30 mm | 840 | Solid | $15.00 | 12 |
2282 | Plate | 25.40 mm | 25.40 mm | 0.42 mm | 840 | Solid | $25.00 | 19 |
2339 | Plate | 9.90 mm | 9.60 mm | 0.30 mm | 840 | Insulation Band | $13.00 | 33 |
2284 | Plate | 30.00 mm | 20.00 mm | 1.00 mm | 840 | Solid | $25.00 | 10 |
2477 | Plate | 38.00 mm | 13.50 mm | 5.00 mm | 840 | Solid | $16.00 | 18 |
1659 | Plate | 40.00 mm | 2.80 mm | 0.80 mm | 840 | Solid | $34.00 | 16 |
1661 | Plate | 40.00 mm | 1.85 mm | 0.60 mm | 840 | Solid | $34.00 | 31 |
1653 | Plate | 43.00 mm | 10.00 mm | 1.40 mm | 840 | Solid | $34.00 | 62 |
2286 | Plate | 50.00 mm | 4.00 mm | 2.70 mm | 840 | Solid | $34.00 | 7 |
2285 | Plate | 50.00 mm | 4.00 mm | 2.60 mm | 840 | Solid | $34.00 | 30 |
2287 | Plate | 50.20 mm | 4.00 mm | 2.70 mm | 840 | Solid | $34.00 | 7 |
2288 | Plate | 50.20 mm | 4.10 mm | 2.70 mm | 840 | Solid | $34.00 | 14 |
2289 | Plate | 50.30 mm | 4.10 mm | 2.70 mm | 840 | Solid | $34.00 | 5 |
1277 | Plate | 59.90 mm | 10.00 mm | 0.80 mm | 840 | Solid | $52.00 | 8 |
1675 | Plate | 60.00 mm | 10.00 mm | 0.32 mm | 840 | Solid | $52.00 | 5 |
346 | Plate | 4.00 mm | 4.00 mm | 1.00 mm | 841 | Solid | $10.00 | 15 |
1822 | Plate | 5.00 mm | 2.00 mm | 0.22 mm | 841 | Solid | $12.00 | 55 |
347 | Plate | 5.00 mm | 5.00 mm | 2.00 mm | 841 | Solid | $12.00 | 54 |
2189 | Plate | 5.00 mm | 5.00 mm | 0.52 mm | 841 | Solid | $12.00 | 67 |
2348 | Plate | 5.00 mm | 2.50 mm | 0.35 mm | 841 | Solid | $12.00 | 190 |
1819 | Plate | 6.00 mm | 6.00 mm | 1.10 mm | 841 | Solid | $12.00 | 112 |
2350 | Plate | 6.00 mm | 6.00 mm | 1.00 mm | 841 | Solid | $12.00 | 178 |
2349 | Plate | 6.00 mm | 3.10 mm | 1.10 mm | 841 | Solid | $12.00 | 89 |
2353 | Plate | 6.30 mm | 4.40 mm | 1.00 mm | 841 | Solid | $12.00 | 104 |
2354 | Plate | 6.40 mm | 4.50 mm | 1.00 mm | 841 | Solid | $12.00 | 377 |
1816 | Plate | 6.40 mm | 4.40 mm | 1.00 mm | 841 | Solid | $12.00 | 1075 |
2356 | Plate | 7.00 mm | 7.00 mm | 0.22 mm | 841 | Solid | $12.00 | 41 |
2357 | Plate | 8.00 mm | 3.00 mm | 1.00 mm | 841 | Wrap Around | $13.00 | 143 |
2358 | Plate | 8.00 mm | 8.00 mm | 0.51 mm | 841 | Wrap Around | $13.00 | 29 |
2371 | Plate | 10.00 mm | 10.00 mm | 0.50 mm | 841 | Wrap Around | $13.00 | 9 |
2193 | Plate | 15.00 mm | 3.00 mm | 0.52 mm | 841 | Solid | $12.00 | 5 |
1391 | Plate | 16.10 mm | 5.10 mm | 0.52 mm | 841 | Solid | $12.00 | 10 |
1076 | Plate | 16.50 mm | 5.00 mm | 0.25 mm | 841 | Solid | $12.00 | 155 |
2360 | Plate | 20.00 mm | 10.00 mm | 4.10 mm | 841 | Wrap Around | $16.00 | 10 |
2361 | Plate | 20.10 mm | 10.00 mm | 4.10 mm | 841 | Wrap Around | $16.00 | 6 |
2364 | Plate | 25.00 mm | 25.00 mm | 4.50 mm | 841 | Solid | $25.00 | 18 |
2366 | Plate | 25.40 mm | 25.40 mm | 0.50 mm | 841 | Solid | $25.00 | 24 |
2340 | Plate | 29.90 mm | 9.50 mm | 0.30 mm | 841 | Insulation Band | $25.00 | 6 |
2191 | Plate | 30.00 mm | 22.00 mm | 0.70 mm | 841 | Solid | $25.00 | 18 |
2363 | Plate | 30.00 mm | 10.00 mm | 0.52 mm | 841 | Solid | $25.00 | 24 |
2365 | Plate | 30.00 mm | 22.00 mm | 0.25 mm | 841 | Solid | $25.00 | 5 |
2362 | Plate | 30.00 mm | 5.00 mm | 1.00 mm | 841 | Wrap Around | $25.00 | 11 |
2199 | Plate | 30.00 mm | 10.00 mm | 0.70 mm | 841 | Wrap Around | $26.00 | 46 |
1384 | Plate | 30.10 mm | 5.00 mm | 0.48 mm | 841 | Wrap Around | $25.00 | 48 |
1387 | Plate | 30.00 mm | 2.00 mm | 1.40 mm | 841 | Wrap Around | $25.00 | 11 |
1386 | Plate | 30.10 mm | 5.10 mm | 0.74 mm | 841 | Wrap Around | $25.00 | 11 |
2370 | Plate | 35.00 mm | 35.00 mm | 1.00 mm | 841 | Solid | $35.00 | 27 |
2352 | Plate | 50.00 mm | 49.90 mm | 2.00 mm | 841 | Solid | $52.00 | 5 |
2369 | Plate | 55.00 mm | 20.00 mm | 1.50 mm | 841 | Wrap Around | $55.00 | 9 |
2368 | Plate | 55.10 mm | 22.10 mm | 1.50 mm | 841 | Wrap Around | $55.00 | 11 |
1813 | Plate | 59.90 mm | 20.90 mm | 1.40 mm | 841 | Wrap Around | $55.00 | 9 |
1812 | Plate | 60.00 mm | 21.00 mm | 1.40 mm | 841 | Wrap Around | $55.00 | 13 |
2367 | Plate | 75.00 mm | 10.50 mm | 0.70 mm | 841 | Wrap Around | $55.00 | 5 |
1811 | Plate | 75.00 mm | 10.40 mm | 1.40 mm | 841 | Wrap Around | $55.00 | 6 |
1087 | Plate | 5.00 mm | 3.00 mm | 3.00 mm | 842 | Solid | $12.00 | 712 |
1086 | Plate | 50.00 mm | 5.00 mm | 6.00 mm | 842 | Solid | $35.00 | 16 |
1803 | Plate | 5.00 mm | 5.00 mm | 0.51 mm | 844 | Solid | $12.00 | 46 |
1795 | Plate | 9.10 mm | 6.00 mm | 1.50 mm | 844 | Solid | $12.00 | 8 |
1778 | Plate | 15.10 mm | 3.00 mm | 0.42 mm | 844 | Solid | $12.00 | 229 |
1797 | Plate | 20.00 mm | 19.80 mm | 0.31 mm | 844 | Solid | $15.00 | 5 |
1802 | Plate | 30.00 mm | 5.00 mm | 0.48 mm | 844 | Wrap Around | $25.00 | 14 |
1779 | Plate | 40.00 mm | 10.00 mm | 0.52 mm | 844 | Solid | $34.00 | 25 |
1800 | Plate | 60.00 mm | 21.00 mm | 0.80 mm | 844 | Wrap Around | $55.00 | 9 |
1799 | Plate | 60.10 mm | 21.00 mm | 0.70 mm | 844 | Wrap Around | $55.00 | 6 |
1760 | Plate | 1.10 mm | 1.00 mm | 8.70 mm | 850 | Solid | $12.00 | 6 |
916 | Plate | 2.00 mm | 2.00 mm | 0.43 mm | 850 | Solid | $12.00 | 451 |
1291 | Plate | 2.50 mm | 2.50 mm | 0.50 mm | 850 | Solid | $12.00 | 695 |
1483 | Plate | 3.00 mm | 3.00 mm | 0.31 mm | 850 | Solid | $12.00 | 54 |
1486 | Plate | 3.20 mm | 3.20 mm | 0.29 mm | 850 | Solid | $12.00 | 67 |
1484 | Plate | 4.00 mm | 4.00 mm | 1.00 mm | 850 | Solid | $12.00 | 530 |
537 | Plate | 3.50 mm | 2.90 mm | 0.60 mm | 850 | Solid | $12.00 | 721 |
667 | Plate | 3.80 mm | 3.80 mm | 0.55 mm | 850 | Solid | $12.00 | 1137 |
535 | Plate | 3.80 mm | 1.60 mm | 0.60 mm | 850 | Solid | $12.00 | 1650 |
536 | Plate | 3.95 mm | 3.95 mm | 1.50 mm | 850 | Solid | $12.00 | 216 |
1750 | Plate | 4.00 mm | 1.80 mm | 1.10 mm | 850 | Solid | $12.00 | 472 |
531 | Plate | 4.00 mm | 4.00 mm | 1.50 mm | 850 | Solid | $12.00 | 647 |
1376 | Plate | 4.00 mm | 4.00 mm | 0.83 mm | 850 | Solid | $12.00 | 17 |
1485 | Plate | 4.00 mm | 4.00 mm | 0.90 mm | 850 | Solid | $12.00 | 568 |
1492 | Plate | 4.00 mm | 4.00 mm | 0.90 mm | 850 | Solid | $12.00 | 8688 |
533 | Plate | 4.35 mm | 4.35 mm | 1.65 mm | 850 | Solid | $12.00 | 1262 |
532 | Plate | 4.35 mm | 4.35 mm | 0.85 mm | 850 | Solid | $12.00 | 1078 |
1491 | Plate | 4.40 mm | 4.40 mm | 0.83 mm | 850 | Solid | $12.00 | 6 |
701 | Plate | 4.70 mm | 1.30 mm | 1.00 mm | 850 | Solid | $12.00 | 27183 |
726 | Plate | 4.80 mm | 1.30 mm | 1.00 mm | 850 | Solid | $12.00 | 1181 |
1369 | Plate | 4.80 mm | 3.20 mm | 0.67 mm | 850 | Solid | $12.00 | 212 |
666 | Plate | 5.00 mm | 4.00 mm | 1.00 mm | 850 | Solid | $12.00 | 1621 |
685 | Plate | 5.00 mm | 3.00 mm | 1.00 mm | 850 | Solid | $12.00 | 424 |
1272 | Plate | 5.00 mm | 1.00 mm | 1.00 mm | 850 | Solid | $12.00 | 5047 |
1494 | Plate | 5.00 mm | 5.00 mm | 0.51 mm | 850 | Solid | $12.00 | 46 |
530 | Plate | 5.00 mm | 4.00 mm | 0.55 mm | 850 | Solid | $12.00 | 179 |
528 | Plate | 5.00 mm | 1.60 mm | 0.20 mm | 850 | Solid | $12.00 | 2489 |
529 | Plate | 5.00 mm | 1.80 mm | 0.56 mm | 850 | Solid | $12.00 | 455 |
1493 | Plate | 6.00 mm | 3.00 mm | 0.72 mm | 850 | Solid | $12.00 | 33 |
1749 | Plate | 6.00 mm | 6.00 mm | 0.32 mm | 850 | Solid | $12.00 | 40 |
522 | Plate | 6.10 mm | 4.30 mm | 2.61 mm | 850 | Solid | $12.00 | 32 |
1371 | Plate | 6.40 mm | 6.30 mm | 0.53 mm | 850 | Solid | $12.00 | 27 |
1071 | Plate | 6.40 mm | 4.90 mm | 0.64 mm | 850 | Solid | $12.00 | 411 |
521 | Plate | 6.40 mm | 6.40 mm | 0.80 mm | 850 | Solid | $12.00 | 6 |
1510 | Plate | 6.70 mm | 1.50 mm | 1.00 mm | 850 | Solid | $12.00 | 29 |
700 | Plate | 6.85 mm | 2.00 mm | 1.00 mm | 850 | Solid | $12.00 | 693 |
1745 | Plate | 7.00 mm | 7.00 mm | 0.50 mm | 850 | Solid | $12.00 | 42 |
1506 | Plate | 7.00 mm | 4.00 mm | 0.52 mm | 850 | Solid | $12.00 | 32 |
728 | Plate | 7.15 mm | 1.55 mm | 1.00 mm | 850 | Solid | $12.00 | 935 |
727 | Plate | 7.45 mm | 1.00 mm | 1.00 mm | 850 | Solid | $12.00 | 921 |
699 | Plate | 7.50 mm | 1.00 mm | 1.00 mm | 850 | Solid | $12.00 | 1836 |
503 | Plate | 8.00 mm | 4.00 mm | 0.44 mm | 850 | Solid | $12.00 | 79 |
1490 | Plate | 8.00 mm | 4.00 mm | 0.53 mm | 850 | Solid | $12.00 | 49 |
693 | Plate | 8.00 mm | 3.00 mm | 1.00 mm | 850 | Solid | $12.00 | 3525 |
723 | Plate | 8.90 mm | 5.40 mm | 1.10 mm | 850 | Solid | $12.00 | 54 |
1742 | Plate | 9.00 mm | 8.00 mm | 0.51 mm | 850 | Solid | $12.00 | 63 |
1482 | Plate | 9.00 mm | 8.00 mm | 0.84 mm | 850 | Solid | $12.00 | 64 |
1727 | Plate | 9.00 mm | 8.00 mm | 0.56 mm | 850 | Solid | $12.00 | 706 |
672 | Plate | 9.00 mm | 4.00 mm | 1.00 mm | 850 | Solid | $12.00 | 22 |
881 | Plate | 9.00 mm | 4.00 mm | 3.00 mm | 850 | Solid | $12.00 | 61 |
502 | Plate | 9.40 mm | 4.30 mm | 2.60 mm | 850 | Solid | $12.00 | 89 |
550 | Plate | 9.60 mm | 9.60 mm | 0.60 mm | 850 | Solid | $12.00 | 5 |
688 | Plate | 10.00 mm | 2.00 mm | 1.00 mm | 850 | Solid | $12.00 | 551 |
689 | Plate | 10.00 mm | 1.00 mm | 1.00 mm | 850 | Solid | $12.00 | 1501 |
1380 | Plate | 10.00 mm | 9.00 mm | 0.53 mm | 850 | Solid | $12.00 | 43 |
1754 | Plate | 10.00 mm | 9.00 mm | 0.80 mm | 850 | Solid | $12.00 | 39 |
1707 | Plate | 10.00 mm | 8.00 mm | 1.00 mm | 850 | Solid | $12.00 | 128 |
725 | Plate | 10.00 mm | 1.80 mm | 1.00 mm | 850 | Solid | $12.00 | 788 |
1743 | Plate | 10.00 mm | 8.00 mm | 0.90 mm | 850 | Solid | $12.00 | 14 |
1381 | Plate | 10.00 mm | 6.00 mm | 1.00 mm | 850 | Solid | $12.00 | 35 |
1495 | Plate | 10.00 mm | 7.00 mm | 0.52 mm | 850 | Solid | $12.00 | 13 |
915 | Plate | 10.00 mm | 1.60 mm | 1.00 mm | 850 | Solid | $12.00 | 1031 |
512 | Plate | 10.00 mm | 3.00 mm | 1.00 mm | 850 | Solid | $12.00 | 32 |
690 | Plate | 10.00 mm | 1.60 mm | 1.00 mm | 850 | Solid | $12.00 | 2184 |
1738 | Plate | 10.00 mm | 10.00 mm | 0.80 mm | 850 | Solid | $12.00 | 33 |
566 | Plate | 10.00 mm | 2.50 mm | 1.00 mm | 850 | Solid | $12.00 | 53 |
1748 | Plate | 10.00 mm | 10.00 mm | 0.52 mm | 850 | Solid | $12.00 | 10 |
1132 | Plate | 10.00 mm | 5.00 mm | 0.70 mm | 850 | Solid | $12.00 | 11 |
1379 | Plate | 10.00 mm | 6.00 mm | 0.52 mm | 850 | Solid | $12.00 | 28 |
548 | Plate | 10.00 mm | 7.00 mm | 1.00 mm | 850 | Solid | $12.00 | 10 |
1481 | Plate | 10.10 mm | 5.00 mm | 0.70 mm | 850 | Solid | $12.00 | 107 |
1508 | Plate | 10.50 mm | 4.80 mm | 0.21 mm | 850 | Solid | $12.00 | 76 |
627 | Plate | 11.00 mm | 5.00 mm | 1.00 mm | 850 | Solid | $12.00 | 20 |
1726 | Plate | 11.60 mm | 10.10 mm | 0.70 mm | 850 | Wrap Around | $15.00 | 66 |
724 | Plate | 12.70 mm | 3.80 mm | 1.30 mm | 850 | Solid | $12.00 | 64 |
498 | Plate | 12.70 mm | 2.50 mm | 0.76 mm | 850 | Solid | $12.00 | 41 |
2377 | Plate | 13.00 mm | 6.00 mm | 3.00 mm | 850 | Insulation Band | $12.00 | 53 |
496 | Plate | 13.00 mm | 3.00 mm | 0.30 mm | 850 | Solid | $12.00 | 131 |
1500 | Plate | 13.00 mm | 2.00 mm | 0.32 mm | 850 | Solid | $12.00 | 61 |
1706 | Plate | 14.00 mm | 14.00 mm | 0.80 mm | 850 | Solid | $12.00 | 68 |
1751 | Plate | 14.00 mm | 8.00 mm | 0.52 mm | 850 | Solid | $12.00 | 17 |
1365 | Plate | 14.00 mm | 12.00 mm | 1.00 mm | 850 | Solid | $12.00 | 11 |
490 | Plate | 15.00 mm | 10.00 mm | 1.00 mm | 850 | Solid | $12.00 | 43 |
495 | Plate | 15.00 mm | 5.00 mm | 0.50 mm | 850 | Solid | $12.00 | 41 |
691 | Plate | 15.00 mm | 4.50 mm | 0.70 mm | 850 | Solid | $12.00 | 52 |
1747 | Plate | 15.00 mm | 10.00 mm | 0.54 mm | 850 | Solid | $12.00 | 14 |
1724 | Plate | 15.00 mm | 10.00 mm | 0.53 mm | 850 | Solid | $12.00 | 46 |
1733 | Plate | 15.00 mm | 10.00 mm | 0.90 mm | 850 | Solid | $12.00 | 10 |
1723 | Plate | 15.00 mm | 15.00 mm | 0.70 mm | 850 | Solid | $15.00 | 30 |
673 | Plate | 15.00 mm | 8.90 mm | 1.05 mm | 850 | Solid | $12.00 | 67 |
1364 | Plate | 15.50 mm | 5.50 mm | 2.00 mm | 850 | Solid | $12.00 | 42 |
678 | Plate | 15.70 mm | 6.35 mm | 0.70 mm | 850 | Solid | $12.00 | 34 |
679 | Plate | 15.80 mm | 6.35 mm | 0.70 mm | 850 | Solid | $12.00 | 131 |
1505 | Plate | 16.90 mm | 5.00 mm | 0.52 mm | 850 | Solid | $12.00 | 61 |
634 | Plate | 17.00 mm | 6.00 mm | 1.00 mm | 850 | Wrap Around | $15.00 | 115 |
1689 | Plate | 18.00 mm | 10.00 mm | 0.90 mm | 850 | Solid | $15.00 | 42 |
1740 | Plate | 19.00 mm | 8.00 mm | 0.53 mm | 850 | Solid | $12.00 | 66 |
1693 | Plate | 19.00 mm | 19.00 mm | 8.70 mm | 850 | Solid | $15.00 | 13 |
680 | Plate | 19.00 mm | 3.80 mm | 0.43 mm | 850 | Solid | $12.00 | 206 |
622 | Plate | 19.00 mm | 6.40 mm | 0.50 mm | 850 | Solid | $12.00 | 10 |
1363 | Plate | 19.50 mm | 3.50 mm | 2.00 mm | 850 | Solid | $12.00 | 63 |
1741 | Plate | 20.00 mm | 11.00 mm | 0.52 mm | 850 | Solid | $15.00 | 5 |
1479 | Plate | 20.00 mm | 5.00 mm | 6.50 mm | 850 | Solid | $15.00 | 17 |
1711 | Plate | 25.00 mm | 15.00 mm | 0.90 mm | 850 | Solid | $15.00 | 41 |
1730 | Plate | 25.00 mm | 25.00 mm | 0.51 mm | 850 | Solid | $25.00 | 5 |
909 | Plate | 25.35 mm | 12.70 mm | 1.60 mm | 850 | Solid | $15.00 | 39 |
1715 | Plate | 25.40 mm | 25.40 mm | 0.70 mm | 850 | Solid | $25.00 | 10 |
1709 | Plate | 26.60 mm | 26.60 mm | 0.35 mm | 850 | Solid | $25.00 | 72 |
1728 | Plate | 26.70 mm | 26.60 mm | 0.32 mm | 850 | Solid | $25.00 | 8 |
1710 | Plate | 26.70 mm | 26.70 mm | 0.42 mm | 850 | Solid | $25.00 | 17 |
1716 | Plate | 27.00 mm | 6.10 mm | 0.27 mm | 850 | Insulation Band | $25.00 | 64 |
1397 | Plate | 27.00 mm | 10.00 mm | 0.25 mm | 850 | Solid | $25.00 | 111 |
683 | Plate | 28.00 mm | 4.50 mm | 0.70 mm | 850 | Solid | $25.00 | 17 |
1717 | Plate | 30.00 mm | 30.00 mm | 0.53 mm | 850 | Solid | $34.00 | 9 |
645 | Plate | 30.10 mm | 30.10 mm | 1.00 mm | 850 | Solid | $34.00 | 63 |
687 | Plate | 31.50 mm | 1.40 mm | 1.00 mm | 850 | Solid | $15.00 | 103 |
1713 | Plate | 31.60 mm | 10.60 mm | 0.90 mm | 850 | Insulation Band | $15.00 | 5 |
1714 | Plate | 31.70 mm | 10.60 mm | 0.90 mm | 850 | Insulation Band | $15.00 | 5 |
695 | Plate | 31.90 mm | 4.50 mm | 0.50 mm | 850 | Solid | $15.00 | 252 |
686 | Plate | 32.00 mm | 4.50 mm | 0.50 mm | 850 | Solid | $15.00 | 29 |
702 | Plate | 32.00 mm | 1.60 mm | 1.00 mm | 850 | Solid | $15.00 | 3491 |
697 | Plate | 32.50 mm | 1.30 mm | 0.53 mm | 850 | Solid | $15.00 | 63 |
681 | Plate | 40.70 mm | 1.90 mm | 0.55 mm | 850 | Solid | $34.00 | 313 |
660 | Plate | 48.20 mm | 1.90 mm | 0.60 mm | 850 | Solid | $34.00 | 174 |
659 | Plate | 48.30 mm | 2.00 mm | 0.60 mm | 850 | Solid | $34.00 | 176 |
682 | Plate | 48.25 mm | 1.90 mm | 0.60 mm | 850 | Solid | $34.00 | 293 |
1475 | Plate | 49.70 mm | 7.00 mm | 0.51 mm | 850 | Solid | $34.00 | 7 |
1476 | Plate | 49.80 mm | 7.00 mm | 0.51 mm | 850 | Solid | $34.00 | 11 |
1695 | Plate | 49.80 mm | 7.00 mm | 0.80 mm | 850 | Solid | $34.00 | 8 |
1477 | Plate | 49.90 mm | 7.00 mm | 0.51 mm | 850 | Solid | $34.00 | 10 |
1478 | Plate | 50.00 mm | 7.00 mm | 0.51 mm | 850 | Solid | $34.00 | 8 |
694 | Plate | 63.00 mm | 1.40 mm | 1.00 mm | 850 | Solid | $52.00 | 48 |
698 | Plate | 65.00 mm | 1.30 mm | 0.52 mm | 850 | Solid | $52.00 | 44 |
1692 | Plate | 69.90 mm | 12.90 mm | 0.60 mm | 850 | Solid | $52.00 | 27 |
1722 | Plate | 69.90 mm | 12.90 mm | 0.60 mm | 850 | Solid | $52.00 | 35 |
1721 | Plate | 70.00 mm | 13.00 mm | 0.61 mm | 850 | Solid | $52.00 | 9 |
706 | Plate | 70.00 mm | 13.00 mm | 0.70 mm | 850 | Solid | $52.00 | 18 |
735 | Plate | 1.90 mm | 1.90 mm | 1.00 mm | 851 | Solid | $12.00 | 200 |
813 | Plate | 2.00 mm | 1.00 mm | 0.50 mm | 851 | Solid | $12.00 | 5 |
914 | Plate | 4.20 mm | 4.20 mm | 1.60 mm | 851 | Solid | $12.00 | 409 |
806 | Plate | 4.20 mm | 4.20 mm | 0.80 mm | 851 | Solid | $12.00 | 249 |
913 | Plate | 4.50 mm | 4.40 mm | 0.90 mm | 851 | Solid | $12.00 | 87 |
910 | Plate | 5.00 mm | 4.50 mm | 3.00 mm | 851 | Solid | $12.00 | 2093 |
811 | Plate | 5.10 mm | 4.00 mm | 1.00 mm | 851 | Solid | $12.00 | 255 |
805 | Plate | 5.10 mm | 5.10 mm | 0.42 mm | 851 | Solid | $12.00 | 587 |
812 | Plate | 5.10 mm | 3.10 mm | 0.53 mm | 851 | Solid | $12.00 | 119 |
671 | Plate | 7.00 mm | 4.50 mm | 3.05 mm | 851 | Solid | $12.00 | 2620 |
623 | Plate | 7.00 mm | 3.00 mm | 0.60 mm | 851 | Solid | $12.00 | 24 |
620 | Plate | 8.00 mm | 8.00 mm | 0.40 mm | 851 | Solid | $12.00 | 57 |
810 | Plate | 9.00 mm | 8.00 mm | 0.50 mm | 851 | Solid | $12.00 | 39 |
630 | Plate | 10.00 mm | 4.00 mm | 1.00 mm | 851 | Solid | $12.00 | 53 |
804 | Plate | 12.00 mm | 8.00 mm | 0.85 mm | 851 | Solid | $12.00 | 243 |
1107 | Plate | 12.30 mm | 12.10 mm | 0.30 mm | 851 | Other | $12.00 | 9 |
1147 | Plate | 12.30 mm | 6.10 mm | 0.30 mm | 851 | Other | $12.00 | 137 |
815 | Plate | 8.00 mm | 4.90 mm | 1.00 mm | 852 | Solid | $12.00 | 95 |
1075 | Plate | 1.90 mm | 1.90 mm | 0.30 mm | 855 | Solid | $12.00 | 31 |
1969 | Plate | 3.00 mm | 3.00 mm | 0.22 mm | 855 | Solid | $12.00 | 73 |
1080 | Plate | 3.90 mm | 1.75 mm | 1.10 mm | 855 | Solid | $12.00 | 6481 |
912 | Plate | 3.90 mm | 1.75 mm | 1.10 mm | 855 | Solid | $12.00 | 2102 |
172 | Plate | 4.00 mm | 4.00 mm | 0.85 mm | 855 | Solid | $12.00 | 4633 |
1970 | Plate | 4.00 mm | 4.00 mm | 0.50 mm | 855 | Solid | $12.00 | 11 |
1083 | Plate | 4.90 mm | 4.80 mm | 1.00 mm | 855 | Solid | $12.00 | 310 |
1053 | Plate | 6.40 mm | 6.30 mm | 1.20 mm | 855 | Solid | $12.00 | 35 |
1052 | Plate | 6.40 mm | 6.30 mm | 1.10 mm | 855 | Solid | $12.00 | 69 |
911 | Plate | 6.40 mm | 6.40 mm | 1.00 mm | 855 | Solid | $12.00 | 1926 |
1996 | Plate | 8.00 mm | 0.52 mm | 10.10 mm | 855 | Solid | $12.00 | 37 |
1968 | Plate | 9.10 mm | 8.00 mm | 0.50 mm | 855 | Solid | $12.00 | 30 |
1976 | Plate | 12.70 mm | 12.70 mm | 1.00 mm | 855 | Solid | $12.00 | 14 |
1980 | Plate | 12.90 mm | 9.50 mm | 0.40 mm | 855 | Wrap Around | $13.00 | 50 |
1981 | Plate | 13.00 mm | 9.50 mm | 0.40 mm | 855 | Wrap Around | $13.00 | 12 |
1918 | Plate | 13.00 mm | 3.00 mm | 0.32 mm | 855 | Solid | $12.00 | 46 |
1378 | Plate | 13.50 mm | 1.70 mm | 0.28 mm | 855 | Solid | $12.00 | 71 |
2495 | Plate | 14.00 mm | 14.00 mm | 0.80 mm | 855 | Solid | $15.00 | 31 |
2496 | Plate | 14.10 mm | 14.10 mm | 0.80 mm | 855 | Solid | $15.00 | 10 |
1848 | Plate | 15.00 mm | 1.50 mm | 0.52 mm | 855 | Solid | $12.00 | 264 |
1991 | Plate | 15.00 mm | 4.00 mm | 1.00 mm | 855 | Solid | $12.00 | 34 |
1993 | Plate | 15.10 mm | 1.60 mm | 0.52 mm | 855 | Solid | $12.00 | 62 |
1920 | Plate | 15.20 mm | 15.20 mm | 1.30 mm | 855 | Solid | $15.00 | 14 |
2408 | Plate | 24.10 mm | 3.00 mm | 0.27 mm | 855 | Solid | $12.00 | 20 |
2409 | Plate | 24.20 mm | 3.00 mm | 0.22 mm | 855 | Solid | $14.00 | 31 |
2410 | Plate | 24.20 mm | 3.00 mm | 0.27 mm | 855 | Solid | $12.00 | 77 |
1832 | Plate | 25.30 mm | 8.30 mm | 1.60 mm | 855 | Solid | $15.00 | 13 |
1833 | Plate | 25.30 mm | 8.40 mm | 1.60 mm | 855 | Solid | $15.00 | 36 |
2065 | Plate | 25.70 mm | 12.70 mm | 25.70 mm | 855 | Solid | $34.00 | 26 |
1829 | Plate | 30.00 mm | 10.00 mm | 1.00 mm | 855 | Solid | $25.00 | 11 |
1982 | Plate | 30.00 mm | 15.00 mm | 0.51 mm | 855 | Solid | $25.00 | 5 |
1983 | Plate | 30.00 mm | 15.10 mm | 0.51 mm | 855 | Solid | $25.00 | 5 |
1984 | Plate | 30.10 mm | 15.10 mm | 0.51 mm | 855 | Solid | $25.00 | 11 |
1938 | Plate | 39.90 mm | 16.90 mm | 0.51 mm | 855 | Solid | $34.00 | 26 |
1940 | Plate | 39.90 mm | 17.00 mm | 0.51 mm | 855 | Solid | $34.00 | 9 |
1828 | Plate | 60.00 mm | 10.00 mm | 1.00 mm | 855 | Solid | $52.00 | 8 |
1914 | Plate | 69.90 mm | 13.00 mm | 0.70 mm | 855 | Solid | $52.00 | 26 |
1823 | Plate | 70.00 mm | 13.00 mm | 0.70 mm | 855 | Solid | $52.00 | 28 |
1913 | Plate | 69.90 mm | 12.90 mm | 0.62 mm | 855 | Solid | $52.00 | 14 |
1915 | Plate | 70.00 mm | 13.00 mm | 0.62 mm | 855 | Solid | $52.00 | 45 |
1924 | Plate | 71.00 mm | 13.00 mm | 0.60 mm | 855 | Solid | $52.00 | 59 |
1925 | Plate | 71.10 mm | 13.10 mm | 0.60 mm | 855 | Solid | $52.00 | 33 |
2026 | Plate | 1.50 mm | 1.50 mm | 2.10 mm | 880 | Solid | $12.00 | 298 |
2020 | Plate | 2.00 mm | 2.00 mm | 4.00 mm | 880 | Solid | $12.00 | 207 |
2027 | Plate | 2.50 mm | 2.40 mm | 1.30 mm | 880 | Solid | $12.00 | 193 |
2028 | Plate | 2.50 mm | 2.50 mm | 0.45 mm | 880 | Solid | $12.00 | 86 |
2060 | Plate | 2.60 mm | 2.60 mm | 0.90 mm | 880 | Solid | $12.00 | 443 |
2061 | Plate | 4.10 mm | 2.10 mm | 0.50 mm | 880 | Solid | $12.00 | 770 |
2022 | Plate | 5.00 mm | 5.00 mm | 2.00 mm | 880 | Solid | $12.00 | 37 |
2029 | Plate | 5.00 mm | 5.00 mm | 1.00 mm | 880 | Solid | $12.00 | 99 |
2023 | Plate | 5.50 mm | 3.10 mm | 0.53 mm | 880 | Wrap Around | $13.00 | 94 |
2024 | Plate | 6.40 mm | 4.40 mm | 1.00 mm | 880 | Solid | $12.00 | 110 |
2025 | Plate | 6.40 mm | 4.50 mm | 1.00 mm | 880 | Solid | $12.00 | 105 |
2062 | Plate | 6.40 mm | 4.50 mm | 1.00 mm | 880 | Solid | $12.00 | 1188 |
2064 | Plate | 7.60 mm | 5.70 mm | 1.30 mm | 880 | Solid | $12.00 | 367 |
2063 | Plate | 7.60 mm | 5.80 mm | 1.30 mm | 880 | Solid | $12.00 | 91 |
2446 | Plate | 12.70 mm | 12.70 mm | 1.00 mm | 880 | Wrap Around | $15.00 | 71 |
2445 | Plate | 12.70 mm | 12.70 mm | 1.00 mm | 880 | Solid | $15.00 | 39 |
2447 | Plate | 12.80 mm | 12.70 mm | 0.30 mm | 880 | Wrap Around | $15.00 | 8 |
2448 | Plate | 12.80 mm | 12.80 mm | 0.20 mm | 880 | Wrap Around | $20.00 | 38 |
2449 | Plate | 12.80 mm | 12.80 mm | 0.30 mm | 880 | Wrap Around | $15.00 | 49 |
2018 | Plate | 14.60 mm | 12.70 mm | 0.31 mm | 880 | Solid | $12.00 | 23 |
2010 | Plate | 20.00 mm | 3.00 mm | 0.25 mm | 880 | Solid | $15.00 | 58 |
2077 | Plate | 20.10 mm | 10.00 mm | 4.50 mm | 880 | Wrap Around | $16.00 | 22 |
2031 | Plate | 25.40 mm | 25.30 mm | 0.70 mm | 880 | Wrap Around | $26.00 | 7 |
2032 | Plate | 25.40 mm | 25.40 mm | 0.70 mm | 880 | Wrap Around | $26.00 | 8 |
2450 | Plate | 25.40 mm | 25.40 mm | 1.00 mm | 880 | Wrap Around | $15.00 | 19 |
2040 | Plate | 25.40 mm | 25.40 mm | 2.80 mm | 880 | Solid | $25.00 | 10 |
2033 | Plate | 25.40 mm | 25.40 mm | 0.70 mm | 880 | Wrap Around | $26.00 | 28 |
2034 | Plate | 25.40 mm | 25.40 mm | 1.00 mm | 880 | Wrap Around | $26.00 | 143 |
2035 | Plate | 25.40 mm | 25.40 mm | 1.40 mm | 880 | Wrap Around | $26.00 | 5 |
2451 | Plate | 25.40 mm | 25.40 mm | 1.10 mm | 880 | Wrap Around | $15.00 | 15 |
2044 | Plate | 25.50 mm | 25.50 mm | 2.80 mm | 880 | Wrap Around | $26.00 | 23 |
1851 | Plate | 28.00 mm | 24.00 mm | 2.50 mm | 880 | Solid | $25.00 | 5 |
2012 | Plate | 30.00 mm | 20.00 mm | 0.43 mm | 880 | Solid | $25.00 | 8 |
2045 | Plate | 30.00 mm | 5.00 mm | 0.60 mm | 880 | Wrap Around | $25.00 | 10 |
2014 | Plate | 30.00 mm | 15.00 mm | 0.31 mm | 880 | Solid | $25.00 | 17 |
2013 | Plate | 30.00 mm | 20.00 mm | 0.53 mm | 880 | Solid | $25.00 | 6 |
2016 | Plate | 30.00 mm | 15.00 mm | 0.53 mm | 880 | Solid | $25.00 | 8 |
2015 | Plate | 30.00 mm | 15.00 mm | 0.43 mm | 880 | Solid | $25.00 | 11 |
2076 | Plate | 37.00 mm | 9.00 mm | 1.80 mm | 880 | Wrap Around | $34.00 | 45 |
2075 | Plate | 37.10 mm | 9.00 mm | 1.80 mm | 880 | Wrap Around | $34.00 | 26 |
2046 | Plate | 38.00 mm | 38.00 mm | 1.00 mm | 880 | Wrap Around | $35.00 | 19 |
2048 | Plate | 38.10 mm | 38.00 mm | 1.00 mm | 880 | Wrap Around | $35.00 | 5 |
1855 | Plate | 38.10 mm | 38.00 mm | 1.10 mm | 880 | Wrap Around | $35.00 | 17 |
1854 | Plate | 38.10 mm | 38.10 mm | 1.00 mm | 880 | Wrap Around | $35.00 | 6 |
2078 | Plate | 40.00 mm | 3.00 mm | 0.25 mm | 880 | Insulation Band | $34.00 | 27 |
2452 | Plate | 50.70 mm | 25.30 mm | 1.00 mm | 880 | Wrap Around | $41.00 | 17 |
2453 | Plate | 50.70 mm | 25.40 mm | 1.00 mm | 880 | Wrap Around | $41.00 | 10 |
2454 | Plate | 76.00 mm | 25.30 mm | 2.00 mm | 880 | Wrap Around | $43.00 | 5 |
2068 | Plate | 76.00 mm | 25.30 mm | 1.00 mm | 880 | Wrap Around | $55.00 | 34 |
2055 | Plate | 76.10 mm | 25.30 mm | 1.00 mm | 880 | Wrap Around | $55.00 | 14 |
2054 | Plate | 76.10 mm | 25.30 mm | 1.00 mm | 880 | Wrap Around | $55.00 | 16 |
2057 | Plate | 76.10 mm | 25.40 mm | 1.00 mm | 880 | Wrap Around | $55.00 | 29 |
2455 | Plate | 76.10 mm | 25.40 mm | 2.00 mm | 880 | Wrap Around | $43.00 | 14 |
1092 | Plate | 6.40 mm | 4.50 mm | 1.00 mm | 881 | Solid | $12.00 | 47 |
1094 | Plate | 10.00 mm | 5.00 mm | 0.75 mm | 881 | Solid | $12.00 | 36 |
1095 | Plate | 10.00 mm | 5.00 mm | 1.00 mm | 881 | Solid | $12.00 | 108 |
1089 | Plate | 44.00 mm | 2.80 mm | 2.10 mm | 881 | Solid | $35.00 | 59 |
707 | Plate | 2.00 mm | 2.00 mm | 1.00 mm | Type 6 | Solid | $13.00 | 1469 |
2492 | Ring | 22.80 mm | 4.10 mm | $17.00 | 8 | |||
2298 | Ring | 9.60 mm | 4.80 mm | 2.00 mm | 481 | Solid | $14.00 | 75 |
1430 | Ring | 6.00 mm | 1.90 mm | 0.21 mm | 840 | Solid | $14.00 | 11 |
1353 | Ring | 8.20 mm | 6.10 mm | 0.80 mm | 840 | Solid | $12.00 | 316 |
2479 | Ring | 8.60 mm | 5.50 mm | 1.50 mm | 840 | Solid | $17.00 | 290 |
2482 | Ring | 9.80 mm | 6.10 mm | 1.50 mm | 840 | Solid | $17.00 | 64 |
2480 | Ring | 9.80 mm | 6.10 mm | 1.50 mm | 840 | Solid | $17.00 | 33 |
2484 | Ring | 9.90 mm | 6.10 mm | 1.60 mm | 840 | Solid | $17.00 | 25 |
2481 | Ring | 9.90 mm | 6.10 mm | 1.60 mm | 840 | Solid | $17.00 | 14 |
2483 | Ring | 9.90 mm | 6.10 mm | 1.50 mm | 840 | Solid | $17.00 | 22 |
1428 | Ring | 10.00 mm | 4.90 mm | 2.00 mm | 840 | Solid | $14.00 | 15 |
1426 | Ring | 10.10 mm | 5.00 mm | 2.00 mm | 840 | Solid | $14.00 | 16 |
921 | Ring | 11.50 mm | 5.00 mm | 1.30 mm | 840 | Solid | $14.00 | 318 |
2478 | Ring | 12.00 mm | 5.10 mm | 0.40 mm | 840 | Solid | $17.00 | 70 |
1429 | Ring | 12.00 mm | 3.50 mm | 3.00 mm | 840 | Solid | $14.00 | 121 |
1434 | Ring | 12.70 mm | 5.20 mm | 2.30 mm | 840 | Solid | $14.00 | 193 |
2270 | Ring | 14.80 mm | 5.80 mm | 4.00 mm | 840 | Solid | $14.00 | 96 |
1405 | Ring | 14.90 mm | 8.50 mm | 0.72 mm | 840 | Wrap Around | $15.00 | 19 |
99 | Ring | 15.00 mm | 6.00 mm | 2.60 mm | 840 | Solid | $14.00 | 1218 |
1438 | Ring | 15.00 mm | 6.90 mm | 3.20 mm | 840 | Solid | $14.00 | 135 |
1407 | Ring | 15.10 mm | 5.00 mm | 0.44 mm | 840 | Insulation Band | $14.00 | 70 |
2336 | Ring | 15.20 mm | 5.00 mm | 0.44 mm | 840 | Insulation Band | $14.00 | 277 |
2269 | Ring | 19.10 mm | 5.60 mm | 2.60 mm | 840 | Insulation Band | $15.00 | 40 |
2266 | Ring | 19.10 mm | 5.70 mm | 2.60 mm | 840 | Insulation Band | $15.00 | 23 |
1359 | Ring | 20.00 mm | 15.60 mm | 0.43 mm | 840 | Wrap Around | $15.00 | 8 |
1425 | Ring | 25.00 mm | 5.20 mm | 1.15 mm | 840 | Solid | $20.00 | 8 |
1437 | Ring | 25.20 mm | 12.00 mm | 4.00 mm | 840 | Solid | $20.00 | 37 |
1421 | Ring | 25.40 mm | 12.50 mm | 6.40 mm | 840 | Solid | $20.00 | 45 |
1420 | Ring | 29.80 mm | 24.80 mm | 5.00 mm | 840 | Solid | $20.00 | 20 |
1418 | Ring | 30.50 mm | 27.00 mm | 4.75 mm | 840 | Solid | $20.00 | 123 |
1431 | Ring | 38.00 mm | 8.10 mm | 1.00 mm | 840 | Solid | $20.00 | 17 |
2271 | Ring | 38.00 mm | 13.20 mm | 6.40 mm | 840 | Insulation Band | $20.00 | 5 |
2272 | Ring | 38.00 mm | 13.10 mm | 6.40 mm | 840 | Insulation Band | $20.00 | 12 |
1419 | Ring | 38.10 mm | 13.00 mm | 3.80 mm | 840 | Solid | $20.00 | 11 |
1417 | Ring | 38.50 mm | 13.20 mm | 6.40 mm | 840 | Solid | $20.00 | 5 |
2290 | Ring | 4.90 mm | 2.50 mm | 1.00 mm | 841 | Solid | $14.00 | 27 |
2291 | Ring | 5.00 mm | 2.50 mm | 1.00 mm | 841 | Solid | $14.00 | 19 |
2292 | Ring | 5.00 mm | 3.10 mm | 0.51 mm | 841 | Solid | $14.00 | 16 |
2293 | Ring | 6.40 mm | 1.70 mm | 2.00 mm | 841 | Solid | $14.00 | 101 |
2294 | Ring | 7.90 mm | 3.10 mm | 0.60 mm | 841 | Solid | $14.00 | 15 |
1640 | Ring | 8.00 mm | 2.20 mm | 0.70 mm | 841 | Solid | $12.00 | 86 |
1050 | Ring | 8.00 mm | 4.40 mm | 2.00 mm | 841 | Solid | $14.00 | 2903 |
2295 | Ring | 8.10 mm | 4.10 mm | 1.00 mm | 841 | Solid | $14.00 | 85 |
571 | Ring | 8.00 mm | 5.00 mm | 2.00 mm | 841 | Solid | $14.00 | 17 |
2296 | Ring | 9.20 mm | 3.20 mm | 1.00 mm | 841 | Solid | $14.00 | 1093 |
2297 | Ring | 9.50 mm | 4.80 mm | 2.00 mm | 841 | Solid | $14.00 | 149 |
1638 | Ring | 9.50 mm | 4.90 mm | 2.00 mm | 841 | Solid | $14.00 | 863 |
871 | Ring | 9.90 mm | 4.90 mm | 1.00 mm | 841 | Solid | $14.00 | 312 |
878 | Ring | 9.90 mm | 5.00 mm | 1.00 mm | 841 | Solid | $14.00 | 475 |
2300 | Ring | 10.00 mm | 4.90 mm | 2.00 mm | 841 | Solid | $14.00 | 21 |
1624 | Ring | 10.00 mm | 4.00 mm | 1.00 mm | 841 | Solid | $14.00 | 83 |
2301 | Ring | 10.00 mm | 4.10 mm | 2.00 mm | 841 | Solid | $14.00 | 15 |
1427 | Ring | 10.10 mm | 5.00 mm | 2.00 mm | 841 | Solid | $14.00 | 35 |
2299 | Ring | 10.10 mm | 4.90 mm | 1.00 mm | 841 | Solid | $14.00 | 860 |
2302 | Ring | 11.00 mm | 5.10 mm | 2.50 mm | 841 | Solid | $14.00 | 7 |
2303 | Ring | 11.40 mm | 5.00 mm | 1.30 mm | 841 | Solid | $14.00 | 220 |
2304 | Ring | 11.40 mm | 5.10 mm | 1.30 mm | 841 | Solid | $14.00 | 671 |
870 | Ring | 11.50 mm | 4.90 mm | 1.50 mm | 841 | Solid | $14.00 | 17 |
869 | Ring | 11.50 mm | 5.00 mm | 1.30 mm | 841 | Solid | $14.00 | 3248 |
2307 | Ring | 11.60 mm | 5.20 mm | 1.30 mm | 841 | Solid | $14.00 | 30 |
2305 | Ring | 11.60 mm | 5.10 mm | 2.00 mm | 841 | Solid | $14.00 | 47 |
2306 | Ring | 11.70 mm | 5.10 mm | 2.00 mm | 841 | Solid | $14.00 | 33 |
1634 | Ring | 12.00 mm | 4.70 mm | 2.00 mm | 841 | Solid | $14.00 | 244 |
2308 | Ring | 12.60 mm | 5.20 mm | 2.30 mm | 841 | Solid | $14.00 | 608 |
1633 | Ring | 12.70 mm | 5.20 mm | 2.30 mm | 841 | Solid | $14.00 | 147 |
1632 | Ring | 12.80 mm | 5.00 mm | 2.30 mm | 841 | Solid | $14.00 | 85 |
2374 | Ring | 13.10 mm | 8.20 mm | 0.50 mm | 841 | Wrap Around | $15.00 | 11 |
2373 | Ring | 13.20 mm | 8.20 mm | 0.50 mm | 841 | Wrap Around | $15.00 | 13 |
1623 | Ring | 13.20 mm | 8.10 mm | 0.52 mm | 841 | Solid | $14.00 | 102 |
1636 | Ring | 14.10 mm | 6.40 mm | 4.00 mm | 841 | Solid | $14.00 | 41 |
1620 | Ring | 14.80 mm | 3.60 mm | 5.00 mm | 841 | Solid | $14.00 | 23 |
2187 | Ring | 15.00 mm | 4.00 mm | 2.50 mm | 841 | Solid | $14.00 | 250 |
1619 | Ring | 14.90 mm | 3.60 mm | 5.00 mm | 841 | Solid | $14.00 | 26 |
873 | Ring | 14.90 mm | 3.70 mm | 2.50 mm | 841 | Solid | $14.00 | 103 |
1631 | Ring | 15.00 mm | 3.70 mm | 5.00 mm | 841 | Solid | $14.00 | 217 |
2310 | Ring | 15.80 mm | 6.50 mm | 2.50 mm | 841 | Solid | $14.00 | 180 |
1639 | Ring | 15.80 mm | 6.70 mm | 2.50 mm | 841 | Solid | $14.00 | 330 |
2462 | Ring | 17.80 mm | 7.80 mm | 3.00 mm | 841 | Solid | $18.00 | 44 |
2463 | Ring | 17.90 mm | 7.80 mm | 3.00 mm | 841 | Solid | $18.00 | 79 |
2312 | Ring | 19.10 mm | 12.90 mm | 0.25 mm | 841 | Solid | $14.00 | 62 |
1627 | Ring | 19.20 mm | 7.30 mm | 5.00 mm | 841 | Solid | $14.00 | 7 |
2309 | Ring | 19.90 mm | 8.10 mm | 2.00 mm | 841 | Solid | $14.00 | 13 |
2311 | Ring | 19.90 mm | 7.90 mm | 4.00 mm | 841 | Tab | $15.00 | 9 |
1637 | Ring | 20.00 mm | 10.00 mm | 5.00 mm | 841 | Solid | $14.00 | 15 |
1629 | Ring | 20.10 mm | 6.20 mm | 4.00 mm | 841 | Solid | $14.00 | 18 |
1612 | Ring | 25.20 mm | 12.40 mm | 6.40 mm | 841 | Solid | $20.00 | 33 |
1628 | Ring | 25.20 mm | 7.00 mm | 4.00 mm | 841 | Solid | $20.00 | 27 |
2313 | Ring | 25.40 mm | 9.50 mm | 3.20 mm | 841 | Solid | $20.00 | 32 |
2464 | Ring | 26.00 mm | 5.00 mm | 6.00 mm | 841 | Solid | $22.00 | 14 |
1618 | Ring | 30.50 mm | 26.90 mm | 4.80 mm | 841 | Solid | $20.00 | 34 |
2273 | Ring | 35.00 mm | 12.50 mm | 0.45 mm | 841 | Solid | $20.00 | 17 |
2425 | Ring | 38.10 mm | 12.80 mm | 0.80 mm | 841 | Solid | $23.00 | 12 |
2314 | Ring | 38.10 mm | 15.70 mm | 5.00 mm | 841 | Solid | $20.00 | 5 |
2315 | Ring | 38.30 mm | 15.70 mm | 5.00 mm | 841 | Solid | $20.00 | 5 |
2318 | Ring | 39.80 mm | 14.80 mm | 5.50 mm | 841 | Solid | $23.00 | 5 |
1617 | Ring | 40.10 mm | 11.10 mm | 5.00 mm | 841 | Solid | $23.00 | 9 |
1616 | Ring | 40.30 mm | 11.10 mm | 5.00 mm | 841 | Solid | $23.00 | 5 |
1615 | Ring | 40.40 mm | 11.10 mm | 5.00 mm | 841 | Solid | $23.00 | 7 |
1578 | Ring | 46.00 mm | 16.00 mm | 6.40 mm | 841 | Insulation Band | $23.00 | 72 |
1574 | Ring | 46.00 mm | 15.90 mm | 5.10 mm | 841 | Solid | $23.00 | 36 |
829 | Ring | 7.50 mm | 4.40 mm | 2.00 mm | 842 | Solid | $14.00 | 12 |
849 | Ring | 14.00 mm | 6.35 mm | 4.00 mm | 842 | Insulation Band | $15.00 | 95 |
827 | Ring | 18.90 mm | 6.30 mm | 5.10 mm | 842 | Solid | $14.00 | 6 |
2241 | Ring | 37.90 mm | 16.00 mm | 5.20 mm | 842 | Insulation Band | $20.00 | 100 |
1807 | Ring | 5.10 mm | 2.20 mm | 0.51 mm | 844 | Solid | $14.00 | 29 |
1772 | Ring | 9.90 mm | 5.00 mm | 1.00 mm | 844 | Solid | $14.00 | 75 |
918 | Ring | 10.00 mm | 5.00 mm | 1.00 mm | 844 | Solid | $14.00 | 317 |
1773 | Ring | 10.00 mm | 5.10 mm | 2.00 mm | 844 | Solid | $14.00 | 11 |
1768 | Ring | 10.00 mm | 5.10 mm | 1.00 mm | 844 | Solid | $14.00 | 113 |
1808 | Ring | 10.00 mm | 4.90 mm | 4.90 mm | 844 | Solid | $14.00 | 15 |
1781 | Ring | 10.10 mm | 5.00 mm | 4.00 mm | 844 | Solid | $14.00 | 114 |
823 | Ring | 11.40 mm | 5.00 mm | 1.20 mm | 844 | Solid | $14.00 | 10 |
822 | Ring | 11.50 mm | 5.00 mm | 1.25 mm | 844 | Solid | $14.00 | 398 |
1775 | Ring | 11.50 mm | 5.10 mm | 1.30 mm | 844 | Solid | $14.00 | 27 |
1767 | Ring | 11.80 mm | 6.60 mm | 4.00 mm | 844 | Solid | $14.00 | 52 |
1782 | Ring | 12.00 mm | 5.20 mm | 2.70 mm | 844 | Solid | $14.00 | 36 |
1771 | Ring | 12.40 mm | 5.10 mm | 2.30 mm | 844 | Solid | $14.00 | 9 |
1774 | Ring | 12.50 mm | 5.10 mm | 2.30 mm | 844 | Solid | $14.00 | 40 |
1805 | Ring | 12.60 mm | 6.30 mm | 4.10 mm | 844 | Solid | $14.00 | 211 |
1780 | Ring | 12.70 mm | 6.40 mm | 4.10 mm | 844 | Solid | $14.00 | 9 |
1770 | Ring | 12.80 mm | 6.40 mm | 4.10 mm | 844 | Solid | $14.00 | 94 |
1765 | Ring | 12.90 mm | 5.20 mm | 2.30 mm | 844 | Solid | $14.00 | 85 |
1766 | Ring | 13.00 mm | 5.30 mm | 2.30 mm | 844 | Solid | $14.00 | 35 |
9 | Ring | 12.70 mm | 5.10 mm | 2.30 mm | 844 | Solid | $14.00 | 36 |
1769 | Ring | 15.00 mm | 7.00 mm | 4.50 mm | 844 | Solid | $14.00 | 29 |
1806 | Ring | 15.00 mm | 10.70 mm | 0.47 mm | 844 | Solid | $14.00 | 17 |
1762 | Ring | 21.70 mm | 10.10 mm | 4.80 mm | 844 | Solid | $14.00 | 55 |
1756 | Ring | 21.90 mm | 10.10 mm | 4.80 mm | 844 | Solid | $14.00 | 132 |
1764 | Ring | 21.90 mm | 13.20 mm | 3.30 mm | 844 | Solid | $14.00 | 7 |
1758 | Ring | 25.10 mm | 18.50 mm | 12.80 mm | 844 | Solid | $20.00 | 15 |
1621 | Ring | 5.00 mm | 1.40 mm | 25.10 mm | 850 | Solid | $14.00 | 14 |
1362 | Ring | 5.00 mm | 1.30 mm | 1.50 mm | 850 | Solid | $14.00 | 71 |
2376 | Ring | 6.30 mm | 3.20 mm | 0.60 mm | 850 | Solid | $14.00 | 51 |
1602 | Ring | 6.40 mm | 4.40 mm | 0.21 mm | 850 | Solid | $14.00 | 22 |
2385 | Ring | 6.50 mm | 3.20 mm | 0.60 mm | 850 | Solid | $14.00 | 7 |
1610 | Ring | 7.90 mm | 2.70 mm | 1.00 mm | 850 | Solid | $14.00 | 141 |
1622 | Ring | 8.00 mm | 2.30 mm | 0.70 mm | 850 | Solid | $12.00 | 86 |
558 | Ring | 8.80 mm | 3.40 mm | 2.20 mm | 850 | Solid | $14.00 | 93 |
1354 | Ring | 8.90 mm | 3.40 mm | 2.30 mm | 850 | Solid | $12.00 | 100 |
1604 | Ring | 9.40 mm | 3.40 mm | 2.60 mm | 850 | Solid | $14.00 | 76 |
1607 | Ring | 9.50 mm | 3.60 mm | 1.00 mm | 850 | Solid | $14.00 | 81 |
1355 | Ring | 10.00 mm | 3.00 mm | 3.00 mm | 850 | Solid | $14.00 | 86 |
1412 | Ring | 12.50 mm | 4.50 mm | 7.00 mm | 850 | Solid | $15.00 | 26 |
554 | Ring | 12.70 mm | 6.20 mm | 1.60 mm | 850 | Solid | $14.00 | 138 |
848 | Ring | 12.70 mm | 6.40 mm | 1.60 mm | 850 | Solid | $14.00 | 82 |
1413 | Ring | 13.00 mm | 9.90 mm | 1.50 mm | 850 | Solid | $14.00 | 54 |
1416 | Ring | 15.90 mm | 13.10 mm | 1.50 mm | 850 | Solid | $14.00 | 55 |
2375 | Ring | 17.00 mm | 12.90 mm | 3.00 mm | 850 | Solid | $14.00 | 641 |
2380 | Ring | 19.10 mm | 12.90 mm | 0.25 mm | 850 | Solid | $14.00 | 116 |
2381 | Ring | 19.10 mm | 12.50 mm | 0.50 mm | 850 | Solid | $14.00 | 37 |
2379 | Ring | 19.90 mm | 9.80 mm | 1.00 mm | 850 | Solid | $14.00 | 6 |
2382 | Ring | 20.10 mm | 6.50 mm | 2.00 mm | 850 | Solid | $14.00 | 34 |
1414 | Ring | 22.50 mm | 19.50 mm | 1.50 mm | 850 | Solid | $15.00 | 21 |
1411 | Ring | 25.00 mm | 12.40 mm | 2.00 mm | 850 | Solid | $20.00 | 16 |
1606 | Ring | 25.20 mm | 12.80 mm | 6.40 mm | 850 | Solid | $20.00 | 54 |
1605 | Ring | 25.40 mm | 12.70 mm | 6.40 mm | 850 | Solid | $20.00 | 288 |
1408 | Ring | 25.50 mm | 3.00 mm | 1.00 mm | 850 | Solid | $20.00 | 7 |
2383 | Ring | 30.50 mm | 15.20 mm | 2.60 mm | 850 | Solid | $20.00 | 65 |
1804 | Ring | 38.00 mm | 13.10 mm | 6.40 mm | 850 | Solid | $20.00 | 13 |
616 | Ring | 38.00 mm | 12.60 mm | 3.20 mm | 850 | Insulation Band | $20.00 | 440 |
2384 | Ring | 40.00 mm | 19.90 mm | 1.00 mm | 850 | Solid | $20.00 | 14 |
1361 | Ring | 5.90 mm | 3.70 mm | 1.00 mm | 851 | Solid | $14.00 | 31 |
1360 | Ring | 6.50 mm | 2.60 mm | 1.00 mm | 851 | Solid | $12.00 | 115 |
382 | Ring | 15.00 mm | 3.00 mm | 0.50 mm | 851 | Insulation Band | $15.00 | 1930 |
833 | Ring | 20.00 mm | 3.00 mm | 0.28 mm | 851 | Insulation Band | $15.00 | 133 |
832 | Ring | 22.90 mm | 4.01 mm | 0.40 mm | 851 | Solid | $14.00 | 60 |
1409 | Ring | 24.70 mm | 11.80 mm | 2.00 mm | 851 | Solid | $14.00 | 19 |
1488 | Ring | 25.30 mm | 12.70 mm | 6.40 mm | 851 | Solid | $20.00 | 6 |
1164 | Ring | 38.10 mm | 12.80 mm | 6.40 mm | 851 | Insulation Band | $20.00 | 974 |
2490 | Ring | 5.10 mm | 1.40 mm | 2.00 mm | 855 | Solid | $17.00 | 50 |
1944 | Ring | 7.90 mm | 2.70 mm | 0.70 mm | 855 | Solid | $14.00 | 89 |
2491 | Ring | 8.00 mm | 2.20 mm | 1.00 mm | 855 | Insulation Band | $17.00 | 53 |
1357 | Ring | 11.00 mm | 3.90 mm | 2.00 mm | 855 | Solid | $14.00 | 567 |
1356 | Ring | 11.00 mm | 4.00 mm | 2.00 mm | 855 | Solid | $14.00 | 117 |
1838 | Ring | 11.10 mm | 4.00 mm | 2.00 mm | 855 | Solid | $14.00 | 386 |
1844 | Ring | 12.00 mm | 3.50 mm | 3.00 mm | 855 | Solid | $14.00 | 45 |
1845 | Ring | 12.00 mm | 3.40 mm | 3.00 mm | 855 | Solid | $14.00 | 27 |
2401 | Ring | 12.60 mm | 4.60 mm | 2.60 mm | 855 | Solid | $18.00 | 35 |
1839 | Ring | 14.90 mm | 8.30 mm | 4.00 mm | 855 | Solid | $14.00 | 95 |
1846 | Ring | 16.60 mm | 4.60 mm | 1.00 mm | 855 | Solid | $14.00 | 27 |
2493 | Ring | 22.90 mm | 4.10 mm | 0.40 mm | 855 | Insulation Band | $17.00 | 10 |
2494 | Ring | 23.00 mm | 4.10 mm | 0.40 mm | 855 | Insulation Band | $17.00 | 14 |
2402 | Ring | 25.00 mm | 3.50 mm | 2.50 mm | 855 | Solid | $18.00 | 17 |
1841 | Ring | 25.00 mm | 6.30 mm | 2.50 mm | 855 | Solid | $20.00 | 31 |
2404 | Ring | 25.10 mm | 12.60 mm | 6.40 mm | 855 | Solid | $20.00 | 5 |
2403 | Ring | 25.10 mm | 3.50 mm | 2.50 mm | 855 | Solid | $18.00 | 11 |
2405 | Ring | 25.30 mm | 10.00 mm | 6.00 mm | 855 | Solid | $20.00 | 6 |
1842 | Ring | 25.40 mm | 6.30 mm | 2.50 mm | 855 | Solid | $20.00 | 21 |
2406 | Ring | 25.40 mm | 12.50 mm | 6.40 mm | 855 | Solid | $20.00 | 5 |
1410 | Ring | 27.10 mm | 12.00 mm | 0.72 mm | 855 | Solid | $20.00 | 110 |
1837 | Ring | 38.30 mm | 12.80 mm | 6.40 mm | 855 | Solid | $23.00 | 8 |
1840 | Ring | 49.70 mm | 10.10 mm | 1.00 mm | 855 | Solid | $23.00 | 10 |
2393 | Ring | 68.80 mm | 38.00 mm | 0.50 mm | 855 | Solid | $30.00 | 13 |
2489 | Ring | 69.40 mm | 38.40 mm | 0.50 mm | 855 | Solid | $30.00 | 27 |
2411 | Ring | 5.10 mm | 2.50 mm | 1.00 mm | 880 | Solid | $17.00 | 52 |
854 | Ring | 6.30 mm | 2.70 mm | 2.50 mm | 880 | Solid | $14.00 | 603 |
851 | Ring | 7.50 mm | 4.30 mm | 2.00 mm | 880 | Solid | $14.00 | 871 |
2112 | Ring | 7.80 mm | 4.30 mm | 2.00 mm | 880 | Solid | $14.00 | 107 |
2113 | Ring | 7.90 mm | 4.20 mm | 1.80 mm | 880 | Solid | $14.00 | 290 |
2412 | Ring | 8.00 mm | 3.50 mm | 1.00 mm | 880 | Solid | $17.00 | 245 |
2114 | Ring | 8.20 mm | 4.30 mm | 2.00 mm | 880 | Solid | $14.00 | 160 |
2115 | Ring | 9.40 mm | 5.00 mm | 2.00 mm | 880 | Solid | $14.00 | 19 |
857 | Ring | 9.50 mm | 5.10 mm | 2.00 mm | 880 | Solid | $14.00 | 47 |
2116 | Ring | 9.50 mm | 3.50 mm | 1.00 mm | 880 | Solid | $14.00 | 41 |
2413 | Ring | 9.50 mm | 5.00 mm | 2.00 mm | 880 | Solid | $17.00 | 117 |
2414 | Ring | 9.60 mm | 5.00 mm | 2.00 mm | 880 | Solid | $17.00 | 102 |
2000 | Ring | 10.00 mm | 5.10 mm | 1.00 mm | 880 | Solid | $14.00 | 50 |
852 | Ring | 10.00 mm | 5.00 mm | 2.00 mm | 880 | Solid | $14.00 | 1406 |
1358 | Ring | 10.00 mm | 4.00 mm | 2.00 mm | 880 | Other | $14.00 | 341 |
2117 | Ring | 10.10 mm | 5.10 mm | 2.20 mm | 880 | Solid | $14.00 | 84 |
855 | Ring | 10.20 mm | 5.00 mm | 2.00 mm | 880 | Solid | $14.00 | 4275 |
2118 | Ring | 10.60 mm | 5.20 mm | 1.30 mm | 880 | Solid | $14.00 | 146 |
1998 | Ring | 11.00 mm | 5.30 mm | 1.30 mm | 880 | Solid | $14.00 | 73 |
1999 | Ring | 10.60 mm | 5.20 mm | 1.30 mm | 880 | Solid | $14.00 | 39 |
2119 | Ring | 11.40 mm | 5.10 mm | 1.30 mm | 880 | Solid | $14.00 | 78 |
2416 | Ring | 11.40 mm | 5.00 mm | 1.30 mm | 880 | Solid | $17.00 | 47 |
2415 | Ring | 11.40 mm | 5.00 mm | 3.00 mm | 880 | Solid | $17.00 | 11 |
2418 | Ring | 11.50 mm | 5.00 mm | 3.00 mm | 880 | Solid | $17.00 | 16 |
2419 | Ring | 11.50 mm | 5.10 mm | 1.30 mm | 880 | Solid | $17.00 | 22 |
2120 | Ring | 11.80 mm | 5.20 mm | 2.70 mm | 880 | Solid | $14.00 | 200 |
2122 | Ring | 12.00 mm | 5.10 mm | 2.70 mm | 880 | Solid | $14.00 | 161 |
2121 | Ring | 12.00 mm | 4.80 mm | 2.00 mm | 880 | Solid | $14.00 | 55 |
2123 | Ring | 12.10 mm | 4.80 mm | 2.00 mm | 880 | Solid | $14.00 | 88 |
2124 | Ring | 12.60 mm | 5.20 mm | 2.30 mm | 880 | Solid | $14.00 | 765 |
2417 | Ring | 12.60 mm | 5.50 mm | 3.20 mm | 880 | Solid | $18.00 | 42 |
2125 | Ring | 12.70 mm | 4.90 mm | 3.20 mm | 880 | Solid | $14.00 | 24 |
2126 | Ring | 12.70 mm | 5.20 mm | 2.20 mm | 880 | Solid | $14.00 | 162 |
2420 | Ring | 12.70 mm | 5.10 mm | 2.30 mm | 880 | Solid | $17.00 | 390 |
856 | Ring | 12.70 mm | 4.90 mm | 2.30 mm | 880 | Solid | $14.00 | 11 |
2127 | Ring | 12.90 mm | 5.20 mm | 2.10 mm | 880 | Solid | $14.00 | 373 |
2128 | Ring | 13.00 mm | 5.30 mm | 2.10 mm | 880 | Solid | $14.00 | 74 |
2505 | Ring | 14.50 mm | 10.40 mm | 1.50 mm | 880 | Solid | $17.00 | 52 |
2129 | Ring | 14.80 mm | 5.70 mm | 4.00 mm | 880 | Solid | $14.00 | 35 |
2130 | Ring | 14.90 mm | 7.00 mm | 5.00 mm | 880 | Solid | $14.00 | 5 |
2131 | Ring | 15.00 mm | 3.80 mm | 5.00 mm | 880 | Solid | $14.00 | 34 |
2421 | Ring | 15.10 mm | 7.00 mm | 4.70 mm | 880 | Solid | $18.00 | 9 |
858 | Ring | 15.80 mm | 4.80 mm | 6.35 mm | 880 | Solid | $14.00 | 31 |
2508 | Ring | 15.80 mm | 6.60 mm | 2.50 mm | 880 | Solid | $18.00 | 163 |
2509 | Ring | 15.80 mm | 6.70 mm | 2.50 mm | 880 | Solid | $18.00 | 17 |
2434 | Ring | 15.80 mm | 6.70 mm | 2.50 mm | 880 | Solid | $18.00 | 223 |
2507 | Ring | 15.80 mm | 6.80 mm | 2.50 mm | 880 | Solid | $18.00 | 6 |
2506 | Ring | 15.90 mm | 6.70 mm | 2.50 mm | 880 | Solid | $18.00 | 8 |
2177 | Ring | 15.90 mm | 7.60 mm | 1.30 mm | 880 | Solid | $14.00 | 51 |
2422 | Ring | 15.90 mm | 6.10 mm | 2.50 mm | 880 | Solid | $18.00 | 52 |
2511 | Ring | 16.00 mm | 6.90 mm | 4.60 mm | 880 | Solid | $18.00 | 6 |
2510 | Ring | 16.00 mm | 6.80 mm | 4.50 mm | 880 | Solid | $18.00 | 5 |
2513 | Ring | 16.00 mm | 6.90 mm | 4.50 mm | 880 | Solid | $18.00 | 12 |
2178 | Ring | 16.00 mm | 5.90 mm | 2.60 mm | 880 | Solid | $14.00 | 39 |
2179 | Ring | 16.10 mm | 5.70 mm | 2.50 mm | 880 | Solid | $14.00 | 49 |
2180 | Ring | 16.10 mm | 6.00 mm | 2.50 mm | 880 | Solid | $14.00 | 33 |
2181 | Ring | 17.90 mm | 12.00 mm | 1.10 mm | 880 | Solid | $14.00 | 23 |
2182 | Ring | 18.70 mm | 5.10 mm | 6.50 mm | 880 | Solid | $14.00 | 115 |
2184 | Ring | 18.80 mm | 6.50 mm | 5.60 mm | 880 | Solid | $14.00 | 19 |
2514 | Ring | 18.80 mm | 8.60 mm | 5.10 mm | 880 | Solid | $18.00 | 33 |
2515 | Ring | 18.80 mm | 9.70 mm | 5.10 mm | 880 | Solid | $18.00 | 61 |
2423 | Ring | 18.80 mm | 6.30 mm | 2.60 mm | 880 | Solid | $18.00 | 68 |
860 | Ring | 18.90 mm | 6.40 mm | 2.60 mm | 880 | Solid | $14.00 | 36 |
2517 | Ring | 18.90 mm | 9.70 mm | 5.10 mm | 880 | Solid | $18.00 | 126 |
2185 | Ring | 18.90 mm | 6.40 mm | 5.10 mm | 880 | Solid | $14.00 | 27 |
2518 | Ring | 19.00 mm | 9.70 mm | 5.10 mm | 880 | Solid | $18.00 | 37 |
2519 | Ring | 19.00 mm | 9.80 mm | 5.10 mm | 880 | Solid | $18.00 | 35 |
2424 | Ring | 19.00 mm | 7.50 mm | 1.30 mm | 880 | Solid | $17.00 | 15 |
2133 | Ring | 19.00 mm | 7.70 mm | 3.20 mm | 880 | Solid | $14.00 | 102 |
1499 | Ring | 19.00 mm | 9.30 mm | 5.10 mm | 880 | Solid | $14.00 | 404 |
2134 | Ring | 19.00 mm | 7.70 mm | 1.30 mm | 880 | Solid | $14.00 | 163 |
879 | Ring | 19.00 mm | 7.60 mm | 1.30 mm | 880 | Solid | $14.00 | 198 |
2428 | Ring | 19.10 mm | 9.80 mm | 2.50 mm | 880 | Solid | $18.00 | 18 |
2139 | Ring | 19.10 mm | 9.70 mm | 5.10 mm | 880 | Solid | $14.00 | 72 |
2431 | Ring | 19.10 mm | 9.90 mm | 2.60 mm | 880 | Solid | $18.00 | 34 |
2430 | Ring | 19.10 mm | 9.90 mm | 2.50 mm | 880 | Solid | $18.00 | 41 |
2429 | Ring | 19.10 mm | 9.80 mm | 2.60 mm | 880 | Solid | $18.00 | 6 |
2427 | Ring | 19.10 mm | 7.70 mm | 3.20 mm | 880 | Solid | $18.00 | 22 |
2520 | Ring | 19.11 mm | 9.70 mm | 5.10 mm | 880 | Solid | $18.00 | 7 |
2426 | Ring | 19.10 mm | 7.60 mm | 1.30 mm | 880 | Solid | $17.00 | 15 |
2432 | Ring | 19.10 mm | 10.00 mm | 2.50 mm | 880 | Solid | $18.00 | 8 |
2138 | Ring | 19.10 mm | 9.30 mm | 5.10 mm | 880 | Solid | $14.00 | 218 |
2140 | Ring | 19.10 mm | 9.80 mm | 5.10 mm | 880 | Solid | $14.00 | 48 |
2142 | Ring | 19.20 mm | 9.80 mm | 5.10 mm | 880 | Solid | $14.00 | 97 |
2141 | Ring | 19.30 mm | 9.90 mm | 5.10 mm | 880 | Solid | $14.00 | 6 |
2435 | Ring | 19.70 mm | 9.80 mm | 3.70 mm | 880 | Solid | $18.00 | 8 |
2143 | Ring | 19.70 mm | 9.80 mm | 4.00 mm | 880 | Solid | $14.00 | 14 |
2144 | Ring | 19.80 mm | 9.80 mm | 4.00 mm | 880 | Solid | $14.00 | 46 |
2436 | Ring | 19.90 mm | 8.10 mm | 3.00 mm | 880 | Solid | $18.00 | 49 |
2146 | Ring | 19.90 mm | 9.20 mm | 4.80 mm | 880 | Solid | $14.00 | 84 |
2145 | Ring | 19.90 mm | 7.90 mm | 3.00 mm | 880 | Solid | $14.00 | 7 |
2147 | Ring | 19.90 mm | 9.90 mm | 4.00 mm | 880 | Solid | $14.00 | 53 |
2135 | Ring | 19.90 mm | 8.10 mm | 6.00 mm | 880 | Solid | $14.00 | 6 |
2150 | Ring | 20.00 mm | 7.90 mm | 3.00 mm | 880 | Solid | $14.00 | 18 |
2149 | Ring | 20.00 mm | 7.70 mm | 4.80 mm | 880 | Solid | $14.00 | 25 |
2148 | Ring | 20.00 mm | 7.70 mm | 4.10 mm | 880 | Solid | $14.00 | 81 |
2437 | Ring | 20.00 mm | 8.20 mm | 6.00 mm | 880 | Solid | $18.00 | 6 |
2153 | Ring | 20.00 mm | 9.90 mm | 4.00 mm | 880 | Solid | $14.00 | 12 |
2154 | Ring | 20.10 mm | 10.10 mm | 5.00 mm | 880 | Solid | $14.00 | 48 |
2151 | Ring | 20.10 mm | 10.00 mm | 4.00 mm | 880 | Solid | $14.00 | 32 |
2438 | Ring | 20.10 mm | 8.20 mm | 6.00 mm | 880 | Solid | $18.00 | 17 |
2155 | Ring | 20.20 mm | 10.00 mm | 4.00 mm | 880 | Solid | $14.00 | 12 |
2440 | Ring | 25.00 mm | 12.80 mm | 5.10 mm | 880 | Solid | $19.00 | 39 |
2441 | Ring | 25.00 mm | 12.90 mm | 3.20 mm | 880 | Solid | $18.00 | 9 |
2160 | Ring | 25.10 mm | 12.00 mm | 4.00 mm | 880 | Solid | $20.00 | 94 |
2161 | Ring | 25.20 mm | 11.90 mm | 3.80 mm | 880 | Solid | $20.00 | 5 |
2163 | Ring | 25.40 mm | 11.10 mm | 3.40 mm | 880 | Solid | $20.00 | 34 |
2164 | Ring | 25.40 mm | 12.50 mm | 3.20 mm | 880 | Solid | $20.00 | 10 |
2443 | Ring | 25.40 mm | 10.90 mm | 3.60 mm | 880 | Solid | $18.00 | 21 |
2442 | Ring | 25.40 mm | 10.80 mm | 3.60 mm | 880 | Solid | $18.00 | 19 |
2444 | Ring | 25.50 mm | 10.80 mm | 3.00 mm | 880 | Solid | $24.00 | 42 |
2167 | Ring | 30.00 mm | 12.00 mm | 4.00 mm | 880 | Solid | $20.00 | 34 |
1595 | Ring | 40.00 mm | 20.40 mm | 5.00 mm | 880 | Solid | $20.00 | 20 |
929 | Ring | 40.00 mm | 20.00 mm | 5.00 mm | 880 | Solid | $20.00 | 22 |
2231 | Ring | 50.00 mm | 20.00 mm | 5.00 mm | 880 | Solid | $23.00 | 17 |
2174 | Ring | 40.00 mm | 20.50 mm | 5.00 mm | 880 | Solid | $20.00 | 6 |
2173 | Ring | 40.00 mm | 20.40 mm | 5.00 mm | 880 | Solid | $20.00 | 11 |
1594 | Ring | 40.00 mm | 11.00 mm | 5.00 mm | 880 | Solid | $20.00 | 11 |
931 | Ring | 40.25 mm | 20.00 mm | 5.00 mm | 880 | Solid | $20.00 | 117 |
784 | Ring | 40.60 mm | 20.40 mm | 5.10 mm | 880 | Solid | $20.00 | 156 |
2237 | Ring | 49.40 mm | 19.90 mm | 5.00 mm | 880 | Solid | $23.00 | 12 |
1590 | Ring | 49.40 mm | 19.50 mm | 5.00 mm | 880 | Solid | $23.00 | 12 |
899 | Ring | 7.60 mm | 4.40 mm | 2.00 mm | 881 | Solid | $14.00 | 27 |
898 | Ring | 10.10 mm | 5.00 mm | 2.00 mm | 881 | Solid | $14.00 | 798 |
934 | Ring | 19.00 mm | 6.50 mm | 5.00 mm | 881 | Solid | $14.00 | 1178 |
894 | Ring | 19.00 mm | 7.60 mm | 1.30 mm | 881 | Solid | $14.00 | 80 |
932 | Ring | 19.25 mm | 6.50 mm | 5.00 mm | 881 | Solid | $14.00 | 454 |
897 | Ring | 9.15 mm | 6.40 mm | 2.55 mm | 881 | Solid | $14.00 | 64 |
896 | Ring | 19.80 mm | 8.10 mm | 3.00 mm | 881 | Solid | $14.00 | 82 |
2205 | Ring | 38.00 mm | 16.00 mm | 6.40 mm | Type I | Solid | $20.00 | 28 |
1286 | Ring | 23.80 mm | 14.00 mm | 2.40 mm | Type II | Solid | $14.00 | 43 |
1285 | Ring | 24.00 mm | 14.00 mm | 2.40 mm | Type II | Solid | $14.00 | 16 |
2239 | Ring | 50.00 mm | 20.00 mm | 6.00 mm | Type III | Solid | $23.00 | 1895 |
APC International's Clearance Sale: Piezo Pricing and Delivery That Cannot Be Matched
Discovered by Pierre Curie in the 1880s, piezoelectricity is released by certain substances – such as ceramics – after a particular amount of stress is applied to them. Whether you’re looking for sound production, high voltages of electricity, or the ability to start cigarette lighters, the applications of piezoelectricity are truly endless.
In order to get the most utility out of piezoelectricity, it’s important to use materials of the highest quality. After all, you can’t afford to compromise on the integrity of materials you use if you want to complete projects to the best of your ability.
When you buy piezo materials from APC International, you can buy with the peace of mind that comes with knowing you’re getting the best products on the market. At APC International, each member of our experienced engineering team has years of experience in piezoelectric ceramic design and applications. Together, they work out of a state-of-the-art manufacturing facility producing products that are truly second-to-none.
We’re pleased to offer a wide array of ceramic cylinders, discs, plates and rings – of all shapes and sizes. The best part? A lot of them are on sale, and you can check them out above.
Low Piezo Prices for Quality Materials
Today, businesses in all industries consistently find ways to manage expenses as they try to navigate an uncertain economic climate. We understand that perfectly, which is why we offer a variety of products for prices you won’t find anywhere else.
Our catalog is comprehensive, so be sure to browse it thoroughly to find all of the products that meet your precise piezoelectricity needs.
Our Consistent Customer-Centric Approach to Business
At APC International, we focus on meeting the needs of our customers in each and every transaction. To do so, we often engage in ongoing discussions to make sure we supply the high-quality ceramics of the exact specifications you expect. Depending on your exact specifications, we can also design customized piezo devices for particular applications.
Take Advantage of Our Piezo Prices, Delivery and Customer Service
We pride ourselves on constantly conducting business with integrity and professionalism. We also work on behalf of our customers, striving to anticipate their future needs while immediately responding to the ones they’re currently facing.
Per the terms of this sale, all products will be sold on a first come first serve basis — make sure to get the items you need before supplies are gone! Once you decide to place an order, you’ll get your materials within one week – if not sooner – so you can get to work on your projects quickly.
If you’re looking for piezo prices and delivery that can’t be beat, you’ve come to the right place. Browse our catalog with confidence. And if you have questions, we have answers. Contact us today, and we’ll work together to find the precise piezoelectric ceramic materials you need to meet your goals.
Clearance Sale Terms & Conditions for PZT Piezo Shapes
- All of APC International, Ltd.’s standard terms and conditions apply.
- APC requires a minimum order value of $135.00. Customers may select up to 5 different products to achieve this minimum order value.
- No purchase may leave APC with a quantity of less than 10 pieces. Lots of less than 11 pieces must be purchased in their entirety.
- Final deliverable quantity will be determined by APC following QC inspection.
- Shipping is the responsibility of the buyer, prices above do not include shipping.
- Parts will be sold on a first come first serve basis, availability is not guaranteed.
- Delivery time is one week or sooner, FOB Mackeyville, Pennsylvania, USA.
- For orders of greater than 50 pieces, contact APC for volume discounts.
- If you require a part that is not listed contact APC for a non-clearance quote at [email protected]